Thaum vuam hlau cam khwb cia, kev xaiv electrode yog qhov tseem ceeb rau kev ua tiav cov txiaj ntsig zoo tshaj plaws. Ib qho kev xaiv yog aCasting Vuam Qws, tshwj xeeb tshaj yog GB/T EZNiCu-1 (Z508) electrode. Nrog lub plawv nickel-tooj liab alloy (monel) thiab lub txheej graphitized, lub electrode no zoo tagnrho rau ntau yam kev siv vuam hlau cam khwb cia.
GB/T EZNiCu-1 (Z508) cast electrode yog tsim los muab qhov ruaj khov arc, ua rau nws yooj yim rau kev khiav lag luam hauv ob qho tib si DC thiab AC vuam cov txheej txheem. Lub electrode cov khoom sib xyaw tshwj xeeb thiab nickel-tooj liab alloy core ua rau nws tuaj yeem vuam cov khoom grey cast iron zoo. Lub graphitized txheej txhim kho kev ua tau zoo ntawm lub electrode, ua kom ntseeg tau tias muaj lub vuam du thiab sib xws. Nws yog ib qho tsim nyog sau tseg tias thaum Z508 muaj kev siv tshuab zoo thiab txiav cov khoom, nws tseem muaj qee qhov kev txwv hauv kev tiv thaiv kab nrib pleb thiab lub zog sib koom ua ke.
Ib qho ntawm cov kev siv tseem ceeb ntawm GB/T EZNiCu-1 (Z508)Casting Vuam Qwsyog kho cov khoom siv hlau grey uas tsis muaj zog heev. Qhov no ua rau nws zoo tagnrho rau cov ntawv thov uas qhov sib koom ua ke yuav tsis raug kev ntxhov siab lossis kev thauj khoom loj. Z508 electrode yog qhov tsim nyog tshwj xeeb rau kev sau cov kab nrib pleb lossis qhov tsis zoo hauv cov khoom siv hlau cam khwb cia, muab cov kev daws teeb meem pheej yig los txuas lub neej kev pabcuam ntawm cov khoom no. Vim nws lub zog sib koom ua ke qis, nws tsis pom zoo rau cov ntawv thov thauj khoom hnyav.
Hais txog kev ua tau zoo, GB/T EZNiCu-1 (Z508) cast electrode zoo ib yam li Z308, lwm lub electrode hlau cam khwb cia uas siv ntau. Z508 electrode muaj qhov nrawm dua ntawm cov hlau tso rau hauv, uas ua rau muaj kev pheej hmoo ntawm kev tawg. Cov neeg vuam yuav tsum ua haujlwm nrog kev ceev faj thiab xyuas kom meej tias muaj kev kho ua ntej thiab tom qab vuam kom txo tau cov kev pheej hmoo no. Kev nkag siab txog cov yam ntxwv ntawm Z508 electrode yog qhov tseem ceeb rau kev vuam zoo thiab tswj kev ncaj ncees ntawm cov khoom vuam.
GB/T EZNiCu-1 (Z508)cam khwb cia vuam pas nrigyog ib qho cuab yeej siv tau zoo heev rau cov neeg ua haujlwm hlau grey cast. Nws lub plawv hlau nickel-tooj liab thiab txheej graphitized muab kev paub txog kev vuam ruaj khov uas haum rau ntau yam kev siv. Cov neeg vuam yuav tsum paub txog nws cov kev txwv, tshwj xeeb tshaj yog hais txog lub zog sib koom ua ke thiab kev tiv thaiv tawg. Los ntawm kev nkag siab txog cov yam ntxwv thiab kev siv ntawm Z508 cast welding rod, cov kws tshaj lij tuaj yeem txiav txim siab kom ua tiav cov txiaj ntsig vuam zoo. Txawm hais tias koj kho cov khoom hlau cam khwb cia lossis pib ua haujlwm tshiab, Z508 welding rod yog qhov kev xaiv txhim khu kev qha rau koj cov kev xav tau vuam.