Arc Force hauv Welding yog dab tsi?

Arc Force hauv Welding yog dab tsi?

Lub zog arc yog qhov tshwm sim ntawm kev sib cuam tshuam ntawm kev vuamhluav taws xobthiab cov khoom ua haujlwm. Lub electrode hloov lub zog mus raudaim ntawv ua haujlwm, uas kub thiab yaj. Cov khoom yaj ces khov, tsim ib qho sib txuas.

Qhov ntau ntawm lub zog arc tsim tawm nyob ntawm ntau yam, suav nrog:

  • hom kev vuam siv,
  • qhov loj thiab cov duab ntawm lub electrode,
  • hom hlau uas raug vuam,
  • thiab qhov ceev ntawm kev vuam.

Muaj tej lub sij hawm, lub zog arc yuav loj heev ua rau lub workpiece puas los yog tawg. Yuav kom tiv thaiv qhov no tsis txhob tshwm sim, cov neeg vuam yuav tsum ua tib zoo tswj qhov ntau ntawm lub zog arc uas lawv cov khoom siv vuam tsim tawm. Lawv ua qhov no los ntawm kev kho qhov tam sim no vuam, qhov loj thiab cov duab ntawm electrode, thiab qhov ceev vuam. Los ntawm kev ua tib zoo tswj lub zog arc, cov neeg vuam tuaj yeem tsim cov vuam zoo uas muaj zog thiab tsis muaj qhov tsis zoo.

Yuav siv lub zog arc li cas hauv kev vuam? Lub zog hauv kev vuam yog dab tsi?

Hauv kev vuam, lub zog arc yog siv los tsim ib qho kev sib txuas ntawm ob daim hlau.

Qhov chaw teeb tsa lub zog arc yog dab tsi?

Qhov kev teeb tsa lub zog arc yog qhov ntau ntawm cov hluav taws xob uas siv los vuam. Qhov kev teeb tsa siab dua, qhov hluav taws xob ntau dua thiab qhov hluav taws xob arc ntau dua. Los ntawm kev tswj hwm lub zog arc kom zoo, cov neeg vuam tuaj yeem tsim cov vuam zoo uas muaj zog thiab tsis muaj qhov tsis zoo.

Kub pib thiab arc force yog dab tsi?

Kev pib kub yog ib qho txheej txheem vuam uas siv lub zog arc siab los tsim ib qho sib koom ua ke.

Lub zog arc rau 7018, 6011, thiab 6013 yog dab tsi?

Lub zog arc rau 7018, 6011, thiab 6013 yog txiav txim siab los ntawm hom kev vuam siv, qhov loj thiab cov duab ntawm lub electrode, hom hlau uas raug vuam, thiabvuamceev.

Arc-resistant welding yog dab tsi?

Lub electrode xa lub zog mus rau qhov workpiece hauv arc tsis kam vuam, uas ua kom sov thiab yaj.

 