AWS A5.22 E317LT1-1 Flux CoredArcHlau vuam
JIS Z 3323 TS 317L-FC11
Cov yam ntxwv thiab daim ntawv thov
AWS A5.22 E317LT1-1 Flux Cored Arc Welding Wire yog tsim los rau 100% CO2 roj shielding thiab txhua qhov chaw vuam hlau.
Nws yog siv rau kev sib txuas cov hlau tsis xeb xws li CF -8M thiab CF-3M. Cov hlau vuam ua rau muaj kev ua tau zoo heev ntawm kev tiv thaiv xeb ntawm cov kab nrib pleb. Cov ntawv thov feem ntau suav nrog kev tsim khoom hauv hiav txwv, cov nkoj thauj tshuaj lom neeg nrog rau kev lag luam petro-chemical, pulp thiab ntawv.
Cov Tshuaj Sib Xyaws Ib Txwm Muaj ntawm Cov Hlau Weld (%)
C 0.027 Mn 1.32 Si0.59 P 0.028 S 0.007 Cr 19.20 Ni 13.14 Mo 3.57
Cov Khoom Siv Kho Tshuab Ib Txwm Muaj ntawm Cov Hlau Weld
Lub zog tensile 620MPa Elongation 34%
Cov lus qhia rau kev siv:.
1. Ua ntej vuam, roj, xeb, thiab noo noo yuav tsum tau ntxuav tawm ntawm cov khoom siv uas yuav tsum muaj qhov tsim nyog
kev tiv thaiv los ntawm cua hauv qhov chaw vuam.
2. Siv 99.8% lossis siab dua purity CO2 ua roj tiv thaiv.
3. Khaws cov khoom kom qhuav, thaum nws khaws cia lossis xa tuaj.
Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes,cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.
Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.