Lus piav qhia luv luv:

Ferro-nickel khoom hlau siv rau vuam cam khwb cia hlau thiab hlau hlau.


Product Detail

Khoom cim npe

Nickel AlloyVuam Hlau Tig HlauENiFe-CI

Cov qauv
TS EN ISO 1071 - SC NiFe-1
AWS A5.15 – E NiFe-CI

 

Nta thiab Daim Ntawv Thov

Ferro-npib tsib xeekhoom hlau siv rau vuam cam khwb cia hlau thiab ductile hlau.

Haum rau kev sib koom ua ke ntawm cov hlau cam khwb cia, me me hlau, tsis tshua muaj hlau alloy thiab stainless hlau.

Pom zoo rau welding siab sulfur, phosphorous lossis lubricant-contaminated castings.

Feem ntau yog siv rau ntau yam kev kho thiab tsim cov ntawv thov, suav nrog kev tsim kho cov ncej, lub log, cov pob qij txha tseem ceeb ntawm cov hlau thiab cam khwb cia hlau thiab lwm yam.

Cov khoom siv hauv paus

Grey cam khwb cia hlau, malleable, nodular *
* Cov lus piav qhia, tsis suav nrog cov npe

 

Tshuaj muaj pes tsawg leeg%

C%

Mn%

Si%

P%

S%

   

max

max

max

max

max

   

2.00 Nws

0.80 ib

0.20 ib

0.03 ib

0.03 ib

   

   

Fe%

Ni%

Cu%

Al%

   

rem.

54.00 Nws

max

max

   

56.00 Nws

2.50 Nws

1.00 Nws

   

 

Mechanical Properties
Tensile zog 400-579 MPa  
Yield zog -  
Elongation -  
Kev cuam tshuam lub zog -  

Cov khoom siv tshuab yog kwv yees thiab yuav txawv raws li cov cua sov, tiv thaiv roj, vuam tsis thiab lwm yam.

 

Tiv thaiv Gases

TS EN ISO 14175 - TIG: I1 (Argon)

 

Vuam txoj hauj lwm

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF

 

Cov ntaub ntawv ntim

Txoj kab uas hla

Ntev

Qhov hnyav

1.60 hli

2.40mm 3

3.20 mm

1000 hli

1000 hli

1000 hli

5 Kg

5 Kg

5 Kg