AWS A5.4 E309-16 Stainless Steel Welding Electrode Vuam Khoom Siv Vuam, Vuam Stick

Kev Piav Qhia Luv:

A302 (AWS E309-16) yog Cr23Ni13 stainless hlau electrode nrog titanium-calcium txheej.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Stainless Hlau Vuam Electrode

A302                                      

GB/T E309-16

AWS A5.4 E309-16

Kev piav qhia: A302 yog Cr23Ni13 stainless hlau electrode nrog titanium-calcium txheej. Nws tuaj yeem siv rau ob qho tib si AC thiab DC nrog kev ua haujlwm zoo heev. Cov hlau tso tawm muaj kev tiv thaiv kev tawg thiab kev tiv thaiv oxidation zoo.

Daim Ntawv Thov: Nws yog siv rau kev vuam tib hom hlau tsis xeb, stainless hlau sab hauv, hlau tshwj xeeb (Cr19Ni9 zoo ib yam li cov hlau tsis tshua muaj carbon), hlau chromium siab, hlau manganese siab, thiab lwm yam.

 

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov hlau vuam (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Cov khoom siv kho tshuab ntawm cov hlau vuam:

Khoom sim

Lub zog tensile

Mpa

Kev ntev

%

Tau lees paub

≥550

≥25

 

Pom zoo tam sim no:

Txoj kab uas hla ntawm tus pas nrig

(hli)

2.5

3.2

4.0

5.0

Vuam Tam Sim No

(Ib)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Daim Ntawv Ceeb Toom:

1. Lub electrode yuav tsum tau ci rau 1 teev ntawm 150 ℃ ua ntej vuam ua haujlwm;

2. Vim tias qhov tob ntawm qhov nkag mus rau hauv qhov chaw vuam AC yog qhov tob, yuav tsum siv lub zog DC kom ntau li ntau tau kom nkag mus tob dua. thiab tam sim no yuav tsum tsis txhob loj dhau kom tsis txhob liab ntawm tus pas vuam.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim cov electrodes vuam, cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.


  • Yav dhau los:
  • Tom ntej no: