AWS Chav Kawm E308HT1-1/T1-4 Flux Core Wire Stainless Steel Flux-cored Welding Wire

Kev Piav Qhia Luv:

AWS E308HT1-1/T1-4 Flux Core Wire Daim Ntawv Thov & siv: Cov cuab yeej kho vajtse. Metallurgy. Machinery. Kev Tsim Kho. Shipbuilding. Petroleum. Tshuaj cog. Fais fab sector. Kev Lag Luam Roj.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

AWS Class E308HT1-1/T1-4Flux Core HlauCov Lus Qhia Tshwj Xeeb

Kev faib tawm AWS A5.22, E308HT1-1/T1-4
Daim Ntawv Vuam Flux Core Hlau
Hom Vuam Roj Tiv Thaiv
Txoj kab uas hla .045”, 1/16”
Cov roj tiv thaiv 100% CO2, 75-80% Ar/ sib npaug CO2, 35-50 cfh
Cov Haujlwm Vuam Txhua txoj haujlwm
AWS E308HT1-1/T1-4 Flux Core Wire Daim Ntawv Thov & siv Cov cuab yeej kho vajtse
Kev lag luam hlau
Tshuab
Kev Tsim Kho
Kev tsim nkoj
Roj av
Hoobkas tshuaj lom neeg
Kev lag luam fais fab
Kev Lag Luam Roj Av

AWS Chav Kawm E308HT1-1/T1-4 Flux Core Wire Chemical Composition

C Cr Ni Mo Mn Si P S Cu
0.04 18.0-21.0 9.0-11.0 0.75 0.5-2.5 1.0 0.04 0.03 0.75

AWS Chav Kawm E308HT1-1/T1-4 Flux Core Wire Mechanical Properties

Lub zog tensile, kpsi: 75 feeb
Lub zog tawm los, kpsi: *NWS
Kev ntev %: 30 feeb

Cov Kev Ntsuas Hlau Flux Core AWS Chav Kawm E308HT1-1/T1-4

Txoj kab uas hla Txheej Txheem Volt Cov Amps Cov roj tiv thaiv
in (hli)
.035 (.9) GMAW 26-27 150-165 100% CO2
.045 (1.14) GMAW 26-28 160-200 100% CO2
.063 (1.6) GMAW 27-28 215-250 100% CO2

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes,cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.


  • Yav dhau los:
  • Tom ntej no: