AWS E310T1-1/4 Stainless Steel Flux-cored Vuam Hlau

Kev Piav Qhia Luv:

E310T1-1/4 yog cov hlau flux-cored uas muaj roj tiv thaiv uas tsim los rau kev vuam "txhua qhov chaw" thiab siv tau nrog 75% Ar / 25% CO2 lossis 100% CO2 tiv thaiv roj.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

E310T1-1/4 FLUX-CORED HLUAV TAWG XOV TOOJ

KEV FAIB CAI
AWS 5.22 Chav Kawm E310T1-1/4 / ASME SFA A5.22 Chav Kawm E310T1-1/4
UNS W31031 A#9 F#6

PIAV TXOG
E310T1-1/4 yog cov hlau flux-cored uas muaj roj tiv thaiv uas tsim los rau kev vuam "txhua qhov chaw" thiab siv tau nrog 75% Ar / 25% CO2 lossis 100% CO2 tiv thaiv roj.
Cov kev ntsuas vuam yuav tsum tau ua kom zoo dua kom tsis txhob muaj kev tawg kub.

DAIM NTAWV THOV
E310T1-1 / 4 feem ntau yog siv rau kev vuam cov hlau puag ntawm cov khoom sib xws xws li AISI 310 steels.
E310T1-1 / 4 tuaj yeem siv rau kev vuam cov hlau carbon rau cov hlau tsis xeb.
E310T1-1 / 4 tuaj yeem siv rau kev vuam lossis kho cov taub hau siab alloy thiab cov castings tiv taus corrosion ntawm tib qho kev sib xyaw ua ke.
Siv cov cua sov tsawg - Xav kom siab tshaj plaws 30,000 Joules/In.
Tsis txhob siv cov hlaws dai concave weld
Khaws qhov kub ntawm qhov chaw hla mus rau hauv qab 250 ° F
Sau tag nrho cov qhov pib thiab qhov nres kom tsis txhob muaj cov kab nrib pleb.

TSHUAJ YEEM LI CAS (%)

C Cr Ni Mo Mn Si P S Cu
.10 25.9 20.4 .10 1.4 .82 .015 .005 .08

COV KHOOM SIV TXUJ CI IB TXWM

Lub zog tensile 89,000 PSI
KEV NCAIM MUS HAUV 2” 38%
KEV KHO KUB TSIS MUAJ

Lus Cim: Cov khoom siv kho tshuab tau qhia siv 100% CO2

COV KEV TXHEEJ TXHEEM ZOO TSHAJ PLAWS (siv 100% CO2)

.045” HNUB TIM. Tiaj tiaj & Ntsug Tsuas yog tiaj tiaj xwb
AMPS 130-190 120-250
VOLTS 24-29 25-29
WFS (IPM) 225-450 200-600

LUS CEEV: Nthuav tawm 3/8 "-1/2"
Txo cov volts los ntawm 2 thaum siv 75% Ar / 25% CO2

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes,cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.


  • Yav dhau los:
  • Tom ntej no: