D256 (B-80) Hardfacing Welding Electrode, Surfacing Vuam Qws, Arc Vuam Stick

Kev Piav Qhia Luv:

Lub electrode yooj yim uas tso cov hlau austenitic manganese, uas tawv los ntawm kev hloov pauv txias, siv tau rau cov hlau ntawm tib lub qauv thiab rau cov khoom uas raug kev cuam tshuam loj heev thiab kev sib txhuam nruab nrab.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Hardfacing Vuam Stick ElectrodeRODO P

RODO PARA RECUBRIMIENTO PROTECTOR

Hom Naj Npawb: D256 (B – 80)

Kev Tshuaj Xyuas Hlau Uas Tau Tso Tawm (Cov nqi ib txwm muaj)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Cov yam ntxwv:

Lub electrode yooj yim uas tso cov hlau austenitic manganese, uas tawv los ntawm kev hloov pauv txias, siv tau rau cov hlau ntawm tib lub sib xyaw thiab rau cov khoom uas raug kev cuam tshuam loj heev thiab kev sib txhuam nruab nrab. Nws yog qhov zoo tagnrho rau kev rov qab, txheej thiab kho cov hlau austenitic Mn, cov khoom thiab cov khoom siv hnyav.

 

Cov Khoom Siv Kho Tshuab:Qhov nyuaj 200-250 HB BRINELL thaum tso nyiaj, 300-400 HB Brinell

tom qab ua haujlwm txias hardening.

 

Cov Haujlwm Vuam:Tiaj, Kab rov tav, Saum toj, Ntsug Saum.

 

Tam sim no thiab Polarity:

Rau kev hloov pauv lossis ncaj qha tam sim no

electrode rau tus ncej zoo

ø hli

ø nyob rau hauv

Amperage

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Daim Ntawv Thov: • Siv rau kev sau cov hlau Manganese.

• Kev kho dua tshiab ntawm cov hniav thiab cov thoob khawb av.

• Kev hla thiab lub plawv ntawm cov hlau.

• Cov tshuab zeb thiab rauj zeb.

• Thaum ntaus rauj, nws qhov nyuaj nce mus txog 350 - 400 HB.

• Thaum rov tsim dua lossis rov pleev xim dua, siv AG AR-91 ua lub hauv paus.

• Thaum kub tshaj 300 OC, cov hlau Mn

Lawv pib poob qhov tawv. Cov hlua khi raug pom zoo kom siv

dhia, qhov tsawg kawg nkaus txoj kab uas hla thiab amperage ua tau.

 

 

NTEV: 350 hli.

Qhov hnyav ib lub thawv: 20 kg/44 lbs.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xebvuam electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, tooj dag welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.

 

 

 

 


  • Yav dhau los:
  • Tom ntej no: