E71T-8-H8 A5.20, Carbon Steel Flux Cored Arc Vuam Hlau

Kev Piav Qhia Luv:

E71T-8-H8 yog ib lub hlau carbon uas muaj flux cored thiab muaj cov pa roj carbon uas tiv thaiv tau tus kheej. Nws yog siv rau kev vuam hlau uas tsis muaj cov pa roj carbon thiab qee cov hlau uas tsis muaj hlau sib xyaw uas xav tau kev ua haujlwm zoo heev thaum kub tsawg.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Kev piav qhia:
E71T-8-H8 yog ib lub hlau carbon uas muaj flux cored thiab muaj cov pa roj carbon uas tiv thaiv tau tus kheej. Nws yog siv rau kev vuam uas tsis muaj cov pa roj carbon thiab qee cov hlau uas tsis tshua muaj hlau uas xav tau kev ua haujlwm zoo heev thaum kub tsawg. Cov slag uas khov sai sai ua rau kev vuam yooj yim dua rau txhua qhov chaw. Nws muaj cov duab zoo li lub voj voog, cov duab zoo li lub hlaws dai thiab cov slag uas yooj yim tshem tawm. E71T-8-H8 yog tsim los rau kev siv cov qauv xws li kev tsim choj, kev tsim nkoj thiab kev tsim nkoj me, nrog rau lwm yam kev tsim khoom dav dav.

Kev Faib Pawg & Kev Pom Zoo:
E71T-8-H8 rau AWS A5.20, ASME SFA 5.20
E71T8-A2-CS3-H8 per AWS A5.36, ASME SFA 5.36
AWS D1.8 Kev Tiv Thaiv Av Qeeg, CWB E491T-8-H8, ABS 3YSA, DNV IIIYMS

Cov txiaj ntsig:
Ua haujlwm ntawm qhov ncaj polarity (DCEN) uas tsis muaj roj shielding sab nraud.
Cov slag khov sai ua rau muaj kev sib txuas zoo heev hauv txhua qhov chaw.
Qhia txog kev hloov pauv du, tsawg kawg nkaus spatter thiab yooj yim tshem tawm slag.

Cov Khoom Siv Kho Tshuab Ib Txwm Muaj:
Lub Zog Tensile Kawg (psi) 87,000
Lub zog tawm los (psi) 64,000
Feem Pua Kev Ntev 27

Cov Khoom Muaj Peev Xwm Tso Cia (wt%):
CMnSi P S Al
0.210.720.20 0.010 0.005 0.55

Cov Kev Ntsuas Vuam Pom Zoo (DCEN):

Txoj kab uas hla WFS AMPERAGE HWJ CHIM CTWD (IN.)
1/16″ 120 165 17-18 5/8
  170 200 18-19 xyoo 3/4
  220 235 20-21 1
  270 270 21-22 1
  350 310 23-24 1
         
.072″ 125 185 18-19 xyoo 3/4
  175 220 20-21 1
  200 245 21-23 1
  225 265 22-24 1
  250 275 22-24 1
         
5/64″ 60 140 17-18 3/4
  100 210 18-19 xyoo 3/4
  150 255 21-22 1
  200 300 22-23 1
  250 330 23-24 1

*Cov kev ntsuas no siv tau rau txhua qhov chaw. Lub peev xwm los vuam tawm ntawm qhov chaw ntawm cov theem tam sim no siab dua yuav nyob ntawm qhov tuab ntawm lub phaj thiab kev txawj ntawm tus neeg vuam.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes,cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.


  • Yav dhau los:
  • Tom ntej no: