ER70S-3 Cov Hlau Carbon Steel Vuam Qws, Cov Hlau Sau Rau Cov Hlau Vuam Uas Muaj Roj Tiv Thaiv Arc, Tig thiab Mig Hlau

Kev Piav Qhia Luv:

ER70S3 yog lub hom phiaj dav dav MIG hlau uas tsim nyog rau ntau daim ntawv thov vuam hlau carbon.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

ER70S-3 CARBON STEEL Filler Metals rau Gas Shielded Arc Vuam

ER70S3 yog ib hom hlau MIG dav dav uas tsim nyog rau ntau daim ntawv thov vuam hlau carbon. Nws yog ib hom hlau silicon thiab manganese deoxidized ua rau nws zoo heev rau kev tsim khoom dav dav. Cov khoom no xav tau cov roj tiv thaiv.

Cov Kev Siv: kev tsim khoom dav dav, rooj tog hlau, hlau ntawv, hlau dai kom zoo nkauj, khoom siv ua liaj ua teb

AWS Class: ER70S3 Daim Ntawv Pov Thawj: AWS A5.18/A5.18M:2005
Cov hlau: ER70S3 ASME SFA A5.18

 

Txoj Haujlwm Vuam: F, V, OH, H Tam sim no:
MIG-DCEP
TIG-DCEN

 

Lub zog tensile, kpsi: 70
Lub zog tawm los, kpsi: 58
Kev ntev hauv 2 "%: 22

Cov Khoom Siv Hluav Taws Xob Ib Txwm Muaj Raws Li AWS A5.18 (cov nqi ib qho yog qhov siab tshaj plaws)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Cov Kev Ntsuas Vuam Ib Txwm Muaj
Txoj kab uas hla Txheej Txheem Volt Cov Amps Cov roj tiv thaiv
in (hli)
.035 (0.9) GMAW 28-32 165-200 Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2
.045 (1.2) GMAW 30-34 180-220 Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2
1/16 (1.6) GMAW 30-34 230-260 Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2
.035 (0.9) GMAW 22-25 100-140 Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO2
.045 (1.2) GMAW 23-26 120-150 Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 