Tus nqi Hoobkas Vuam Qws / Vuam Khoom Siv Vuam Electrode (As E6013)

Kev Piav Qhia Luv:

J556 (AWS E8016-G) yog lub electrode hlau uas tsis muaj hlau ntau nrog cov txheej hydrogen potassium tsawg. Ob qho tib si AC thiab DC siv tau, thiab tuaj yeem vuam tau rau txhua qhov chaw.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Ua lub luag haujlwm tag nrho los ua kom tau raws li txhua yam kev xav tau ntawm peb cov neeg yuav khoom; tau txais kev nce qib tas mus li los ntawm kev txhawb nqa kev nce qib ntawm peb cov neeg siv khoom; loj hlob los ua tus khub koom tes kawg ntawm cov neeg siv khoom thiab ua kom muaj kev txaus siab ntawm cov neeg yuav khoom rau Factory Price Welding Rod / Welding Material Welding Electrode (Aws E6013), Peb ib txwm ua kom muaj kev tsim cov khoom tshiab muaj tswv yim los ua kom tau raws li qhov kev thov ntawm peb cov neeg siv khoom thoob plaws ntiaj teb. Koom nrog peb thiab cia peb ua kom kev tsav tsheb muaj kev nyab xeeb dua thiab lom zem dua ua ke!
Ua lub luag haujlwm tag nrho los ua kom tau raws li txhua yam kev xav tau ntawm peb cov neeg siv khoom; tau txais kev nce qib tas mus li los ntawm kev txhawb nqa kev nce qib ntawm peb cov neeg siv khoom; ua tus khub koom tes tas mus li kawg ntawm cov neeg siv khoom thiab ua kom cov neeg siv khoom txaus siab rauTuam Tshoj Vuam Electrode thiab Vuam Qws, Peb cov khoom raug xa tawm thoob ntiaj teb. Peb cov neeg siv khoom yeej ib txwm txaus siab rau peb cov khoom zoo, cov kev pabcuam rau cov neeg siv khoom thiab cov nqi sib tw. Peb lub hom phiaj yog "txuas ntxiv kom tau txais koj txoj kev ntseeg siab los ntawm kev mob siab rau peb txoj kev siv zog rau kev txhim kho peb cov kev daws teeb meem thiab cov kev pabcuam kom ntseeg tau tias peb cov neeg siv khoom kawg, cov neeg siv khoom, cov neeg ua haujlwm, cov neeg muab khoom thiab cov zej zog thoob ntiaj teb uas peb koom tes ua haujlwm".
COV NTAWV THOV:

Vuam cov hlau 9% Cr-1% Mo thiab cov hlau 9% Cr – 2% Mo siv rau lub zog hluav taws xob thiab lub thawv siab.

COV LUS QHIA:

PA-8016-B8 yog lub electrode hydrogen qis uas nws cov hlau vuam muaj 9% Cr-1% Mo. Nws yog tsim los rau cov hlau kub thiab cov hlau rau cov kev pabcuam hydrogen kub, tshwj xeeb tshaj yog hauv kev lag luam petrochemical. Lub electrode tuaj yeem pom zoo rau nws lub zog tensile siab, zoo toughness thiab zoo tiv taus kub.

COV LUS CEEV TXOG KEV SIV:

1. Ua ntej siv, ziab cov electrodes ntawm 350-400°C li ib teev, thiab khaws cov electrodes ntawm 100-150°C tom qab ziab kom qhuav thiab ceev faj kom tsis txhob ntub dej.

2. Siv txoj kev rov qab los yog ntaus lub arc rau ntawm ib lub phaj hlau me me uas tau npaj rau lub hom phiaj tshwj xeeb no kom tiv thaiv cov qhov cua ntawm lub arc pib.

3. Khaws lub arc kom luv li luv tau.

4. Ua kom sov ntawm 100-150 ° C. Qhov kub uas yuav siv sib txawv raws li lub phaj tuab thiab hom hlau uas yuav tsum tau vuam.

5. Ua tib zoo tsis txhob siv cua sov ntau dhau vim tias cua sov ntau dhau ua rau cov hlau vuam puas tsuaj thiab ua rau lub zog vuam puas tsuaj.

IV. COV TSHUAJ YEEM NTAWM COV HLAU WELD (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. COV KHOOM SIV TXUJ CI NTAWM HLAU WELD:

Lub zog Tensile N/mm2(Ksi)

Cov Qoob Loo N/hli2

(Ksi)

Kev ntev%

PWHT

705 (102)

560 (81)

24

740°C x 1 teev

VI. TXOJ HAUJ LWM VUAM: TXHUA TXOJ HAUJ LWM

VII. LOJ THIAB QHOV CHAW UAS POM ZOO (AC/DC+):

Txoj kab uas hla (hli)

2.5

3.2

4.0

5.0

Ntev (hli)

350

350

400

400

Ampere

tiaj tus

55 – 85

90 – 130

130 – 180

180 – 240

V & OH

50 – 80

80 – 115

110 – 170

150 – 200

Ua lub luag haujlwm tag nrho los ua kom tau raws li txhua yam kev xav tau ntawm peb cov neeg yuav khoom; tau txais kev nce qib tas mus li los ntawm kev txhawb nqa kev nce qib ntawm peb cov neeg siv khoom; loj hlob los ua tus khub koom tes kawg ntawm cov neeg siv khoom thiab ua kom muaj kev txaus siab ntawm cov neeg yuav khoom rau Factory Price Welding Rod / Welding Material Welding Electrode (Aws E6013), Peb ib txwm ua kom muaj kev tsim cov khoom tshiab muaj tswv yim los ua kom tau raws li qhov kev thov ntawm peb cov neeg siv khoom thoob plaws ntiaj teb. Koom nrog peb thiab cia peb ua kom kev tsav tsheb muaj kev nyab xeeb dua thiab lom zem dua ua ke!
Nqe HoobkasTuam Tshoj Vuam Electrode thiab Vuam Qws, Peb cov khoom raug xa tawm thoob ntiaj teb. Peb cov neeg siv khoom yeej ib txwm txaus siab rau peb cov khoom zoo, cov kev pabcuam rau cov neeg siv khoom thiab cov nqi sib tw. Peb lub hom phiaj yog "txuas ntxiv kom tau txais koj txoj kev ntseeg siab los ntawm kev mob siab rau peb txoj kev siv zog rau kev txhim kho peb cov kev daws teeb meem thiab cov kev pabcuam kom ntseeg tau tias peb cov neeg siv khoom kawg, cov neeg siv khoom, cov neeg ua haujlwm, cov neeg muab khoom thiab cov zej zog thoob ntiaj teb uas peb koom tes ua haujlwm".