G202 Stainless Steel Welding Electrode, GB/T E410-16 Vuam Rods rau Txhua Txoj Haujlwm

Kev Piav Qhia Luv:

G202 (GB/T E410-16) yog Cr13 stainless hlau electrode nrog titanium calcium txheej. Nws tuaj yeem siv rau txhua qhov chaw vuam nrog AC thiab DC.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Kev vuam hlau tsis xebHluav taws xob

G202                                                     

GB/T E410-16

Kev piav qhia: G202 yog Cr13 stainless hlau electrode nrog titanium calcium txheej. Nws tuaj yeem siv rau txhua qhov chaw vuam nrog AC thiab DC.

Daim Ntawv Thov: Siv rau kev vuam 06Cr13 thiab 12Cr13 stainless hlau qauv, thiab kuj tseem siv tau rau corrosion-resistant thiab hnav-resistant nto surfacing.

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov hlau vuam (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

≤1.0

≤0.90

11.0 ~ 13.5

≤0.7

≤0.75

≤0.75

≤0.03

≤0.04

 

Cov khoom siv kho tshuab ntawm cov hlau vuam:

Khoom sim

Lub zog tensile

Mpa

Kev ntev

%

Tau lees paub

≥450

≥20

 

Pom zoo tam sim no:

Txoj kab uas hla ntawm tus pas nrig

(hli)

3.2

4.0

5.0

Vuam Tam Sim No

(Ib)

80 ~ 120

100 ~ 160

150 ~ 200

Daim Ntawv Ceeb Toom:

1. Lub electrode yuav tsum tau ci rau 1 teev ntawm ib ncig ntawm 150 ℃ ua ntej welding ua haujlwm;

2. Qhov vuam yuav tsum tau preheated rau 250 ~ 350 ° C ua ntej vuam.

 

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.

 

 


  • Yav dhau los:
  • Tom ntej no: