Nta ntawm E6010 Electrode

E6010 Carbon Steel Vuam Electrodes

https://www.tyueweld.com/aws-e6010-mild-steel-welding-electrode-product/

E6010 ectrode yog ib qho yooj yim electrode.Nws yog tsim rau welding low-carbon steel qauv li pipelines, shipbuilding thiab choj, thiab lwm yam.

1. Haum rau DC vuam thiab AC vuam;

2. Lub vuam ceev yog ceev, qhov tob tob yog loj, thiab vuam efficiency siab;

3. Lub vuam seam yog tsim tau zoo, vuam zoo yog siab, thiab vuam seam yog ruaj;

4. Lub slag yog yooj yim tshem tawm, thiab cov slag foams thaum lub sij hawm vuam txheej txheem, uas yog ib qho yooj yim los tswj;

5. Tsim nyog rau kev sib txuas cov hlau muaj zog, xws li txuas hniav, cov hlab ntsha, cov kav dej, thiab lwm yam.

 

Nws yog tsim nyog sau cia tias qhov ntev arc thiab tsim ntawm slag yuav tsum tau tswj kom zoo thaum lub sij hawm vuam txheej txheem E6010, txwv tsis pub, qhov zoo ntawm vuam yuav raug cuam tshuam.Yog li ntawd, cov kev xav tau ntawm kev ua haujlwm yog siab, thiab nws yog ib qho tsim nyog yuav tsum paub txog kev ua haujlwm.

Tshaj tawm los ntawm WENZHOU TIANYU ELECTRONIC CO., LTD.


Post lub sij hawm: Jun-12-2023