Ni327-6 Nickel Alloy Welding Electrodes AWS A5.11 ENiCrMo-6 Vuam Rods, Vuam Cov Qauv Arc Vuam Stick Electrodes

Kev Piav Qhia Luv:

Ni327 -6 (AWS A5.11 ENiCrMo-6) yog ib lub electrode uas siv nickel nrog cov txheej sodium uas muaj hydrogen tsawg. Siv DCEP (direct current electrode positive).


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Nickel thiab Nickel Alloy Vuam Electrode

Ni327-6                                                     

GB/T ENi6620

AWS A5.11 ENiCrMo-6

Kev piav qhia: Ni327 -6 yog ib lub electrode uas muaj nickel nrog cov txheej sodium hydrogen tsawg. Siv DCEP (direct current electrode)zoo). Cov hlau uas tau muab tso rau hauv muaj qhov zoo heev ntawm kev ua kom zoo, kev tawv thiab kev tawg. Cov hlau uas tau muab tso rau hauv muaj cov coefficient nthuav dav zoo ib yam li cov hlau, thiab muaj lub zog siab thiab kev tiv thaiv xeb zoo ntawm qhov kub thiab txias hauv chav tsev.

Daim Ntawv Thov: Nws yog siv rau kev vuam ntawm Ni9% hlau, thiab kuj tseem siv tau rau kev vuam ntawm cov hlau sib txawv thiab cov hlau sib xyaw uas nyuaj rau vuam.

 

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov hlau vuam (%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Lwm yam

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Cov khoom siv kho tshuab ntawm cov hlau vuam:

Khoom sim

Lub zog tensile

Mpa

Lub zog tawm los

Mpa

Kev ntev

%

Tau lees paub

≥620

≥350

≥32

 

Pom zoo tam sim no:

Txoj kab uas hla ntawm tus pas nrig

(hli)

2.5

3.2

4.0

Vuam tam sim no

(Ib)

50 ~ 70

80 ~ 100

110 ~ 150

 

Daim Ntawv Ceeb Toom:

1. Lub electrode yuav tsum tau ci rau 1 teev ntawm ib ncig ntawm 300 ℃ ua ntej vuam ua haujlwm. Sim siv lub arc luv luv los vuam;

2. Nws yog ib qho tseem ceeb uas yuav tsum tau ntxuav cov xeb, roj, dej, thiab cov khoom tsis huv ntawm cov khoom vuam ua ntej vuam.

3. Sim siv lub zog me me ntawm txoj kab thaum vuam, ntau txheej thiab ntau txoj kev vuam.

 

 