Vuam Electrode AWS A5.4 E310Mo-16 Stainless Hlau Vuam Rods Stick Electrodes

Kev Piav Qhia Luv:

A412 (AWS E310Mo-16) yog Cr26Ni21Mo2 ntshiab austenitic stainless hlau electrode nrog titanium calcium txheej.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Kev vuam hlau tsis xebHluav taws xob

A412                                 

GB/T E310Mo-16

AWS A5.4 E310Mo-16

Kev piav qhia: A412 yog Cr26Ni21Mo2 ntshiab austenitic stainless hlau electrode nrog titanium calcium txheej. Nws tuaj yeem siv rau ob qho tib si AC thiab DC nrog kev ua haujlwm zoo heev. Vim tias molybdenum ntxiv rau cov hlau tso, nws qhov kev tiv thaiv pitting, lub zog kub thiab kev tiv thaiv tawg tau zoo dua piv rau A402 thiab A407.

Daim Ntawv Thov: Nws yog siv rau kev vuam cov hlau tsis xeb uas tiv taus cua sov ua haujlwm hauv qhov kub siab, thiab kuj tseem siv tau rau kev vuam cov ntaub thaiv stainless hlau, cov hlau sib txawv, thiab lwm yam. Nws muaj kev tiv thaiv kev tawg zoo dua thaum vuam cov hlau carbon thiab cov hlau tsis tshua muaj zog nrog kev tawv siab.

 

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov hlau vuam (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.030

 

 

Cov khoom siv kho tshuab ntawm cov hlau vuam:

Khoom sim

Lub zog tensile

Mpa

Kev ntev

%

Tau lees paub

≥550

≥25

 

Pom zoo tam sim no:

Txoj kab uas hla ntawm tus pas nrig

(hli)

2.0

2.5

3.2

4.0

5.0

Vuam Tam Sim No

(Ib)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Daim Ntawv Ceeb Toom:

  1. Lub electrode yuav tsum tau ci rau 1 teev ntawm ib ncig ntawm 150 ℃ ua ntej vuam ua haujlwm;
  2. Vim tias qhov tob ntawm qhov nkag mus rau hauv qhov chaw tsis tob thaum lub sijhawm vuam AC, yuav tsum siv lub zog DC kom ntau li ntau tau kom nkag mus tob dua. thiab tam sim no yuav tsum tsis txhob loj dhau kom tsis txhob liab ntawm tus pas vuam.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, cov pas nrig vuam, thiabcov khoom siv vuamtau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.

 

 

 


  • Yav dhau los:
  • Tom ntej no: