AWS A5.23: ECM4 Submerged Arc Welding Wire Welding Consumables Supplier

Kev Piav Qhia Luv:

AWS A5.23: ECM4 Submerged Arc Solid Wire yog ib qho hlau sib xyaw ua ke uas muaj cov hlau tsis sib xyaw ua ke rau kev vuam hauv qab dej hauv cov ntawv thov muaj zog heev. AWS A5.23: ECM4 ua tau raws li AWS A5.23 chemistry M4, thiab yog tsim los rau cov qib tensile siab tshaj 110 ksi.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

PIAV TXOG:

Cov Hlau Uas Muaj Cov Hlau Uas Muaj Cov Hlau Qis

PAWG:

AWS A5.23: ECM4 Submerged Arc Solid Wire yog ib qho hlau sib xyaw ua ke uas muaj cov hlau tsis sib xyaw ua ke rau kev vuam hauv qab dej hauv cov ntawv thov muaj zog heev. AWS A5.23: ECM4 ua tau raws li AWS A5.23 chemistry M4, thiab yog tsim los rau cov qib tensile siab tshaj 110 ksi.

TSEEM CEEB DAIM NTAWV THOV:

Daim ntawv thov ib zaug thiab ntau daim ntawv thov nrog cov submerged arc flux pom zoo, High-Strength Low-Alloy steels, Quench & Tempered steels, Cov khoom siv hnyav, cov khoom siv qauv, lub nkoj hulls, cam khwb cia steels, boiler & pressure vessels

Cov hlau HSLA thiab Q&T

Kev tsim kho vaj tse

Kev tsim khoom ntawm jackup rig

Cov thav duab khoom siv hnyav

Cov nqaj hlau crane

NTA:

Cov hlau-cored hlau tuaj yeem muab cov nqi tso tawm zoo dua piv rau cov hlau khov kho ntawm cov amperages sib piv

Cov xov hlau uas muaj cored muab cov profiles nkag mus dav dua piv rau cov xov hlau khov kho ntawm cov kev sib piv vuam.

Muaj zog heev nrog kev ua kom sov qis zoo heev hauv qhov xwm txheej raws li-welded

Cov kev xav tau ntawm cov tshuaj lom neeg ntawm cov khoom siv vuam yog zoo ib yam li cov ntawm EM4 cov xov hlau khov kho

AWS KEV SIB THAM:

Nrog Flux Mob Cov Lus Qhia Tshwj Xeeb Kev Faib Pawg (Cov Chav Nyob Hauv Tebchaws Meskas) Kev Faib Pawg (SI Units)
SWX 150 Raws li-Welded A5. 23/A5 23M F11A10-ECM4-M4 F76A7-ECM4-M4
Nrog Flux %C % Mn %Si %P %S % Cu % Cr % Ni % Mo %TI+V+Zr
SWX 150 0.06 1.45 0.27 0.012 0.010 0.06 0.31 2.25 0.47 0.02

COV TSHUAJ HMOO NTAWM COV XOV TOOJ LI CAS:

Nrog Flux Cov Hydrogen uas tawg tau
SWX 150 7.5 ml/100g

COV KHOOM SIV TXUJ CI IB TXWM:

Nrog Flux Mob Lub zog tensile Lub Zog Tawm Kev ntev % hauv 2" (50 hli)
SWX 150 Raws li-Welded 113 ksi (779 MPa) 106 ksi (731 MPa) 20%
PWHT* 104 ksi (717 MPa) 97 ksi (669 MPa) 8%

TUS NQI CUAM TSHUAM CHARPY V-NOTCH:

Nrog Flux Mob Qhov nruab nrab ntawm -60°F (-50°C) Qhov nruab nrab ntawm -80°F (-60°C) Qhov nruab nrab ntawm -100°F (-70°C)
SWX 150 Raws li-Welded 55 ft-lbs (75 J) 60 f-bs (81 J) 45 f-Ibs (61 J)
PWHT* 57 f-lbs (77 J) 45 ft-lbs (61 J) —