AWS A5.4 E316L-16 Stainless Hlau Welding Rods

Lus piav qhia luv luv:

A022 (AWS A5.4 E316L-16) is an ultra-low carbon Cr18Ni12Mo2 stainless steel electrode with titanium calcium coating.


Product Detail

Khoom cim npe

Stainless hlau Vuam Electrode

A022                                                 

GB/T E316L-16

AWS E316L-16

Nqe lus piav qhia: A022 yog ib qho ultra-low carbon Cr18Ni12Mo2 stainless hlau electrode nrog titanium calcium txheej.Nws tuaj yeem siv rau AC thiab DC nrog cov txheej txheem ua haujlwm zoo.Cov ntsiab lus carbon ntawm cov hlau deposited yog ≤0.04%, uas muab nws nrog zoo kub tsis kam, corrosion kuj thiab tawg kuj.

 Daim ntawv thov: Nws yog siv rau vuam urea, hluavtaws fiber ntau thiab lwm yam khoom siv thiab tib hom stainless hlau qauv.Nws tseem tuaj yeem siv rau chromium stainless hlau, cov hlau sib xyaw thiab cov hlau tsis sib xws uas tsis tuaj yeem kho cua sov tom qab vuam.

 

Tshuaj muaj pes tsawg leeg ntawm weld hlau (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤ 0.04

0.5 ~ 2.5 hli

≤0.90

17.0-20.0 Nws

11.0 ~ 14.0 Nws

2.0 ~ 3.0 hli

≤ 0.75

≤ 0.030

≤ 0.040

 

Mechanical zog ntawm weld hlau:

Cov khoom kuaj

Tensile zog

Mpa

Elongation

%

lav

≥490

≥30

 

Pom zoo tam sim no:

Qws txoj kab uas hla

(mm)

2.0

2.5

3.2

4.0

5.0

Vuam tam sim no

(A)

25 ~ 50

50 ~ 80

80 ~ 110 ib

110 ~ 160 ib

160-200 Nws

 

Daim ntawv ceeb toom:

1. Cov electrode yuav tsum tau ci rau 1 teev ntawm ib ncig ntawm 150 ℃ ua ntej vuam ua haujlwm;

2. Vim tias qhov nkag mus tob tob yog ntiav thaum lub sij hawm AC vuam, DC fais fab mov yuav tsum tau siv ntau npaum li qhov ua tau kom nkag mus tob dua.thiab tam sim no yuav tsum tsis txhob loj dhau kom tsis txhob muaj qhov liab ntawm lub vuam pas nrig;

3.Qhov corrosion kuj ntawm deposited hlau yog txiav txim los ntawm ob qhov kev pom zoo ntawm cov khoom thiab kev thov.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 


  • Yav dhau los:
  • Tom ntej: