A032Mo (AWS E317L-16) is an ultra-low carbon Cr19Ni13Mo3 stainless steel electrode with titanium calcium coating.


Product Detail

Khoom cim npe

Stainless hlau VuamHluav taws xob

A032 Mo                                            

GB/T E317L-16

AWS E317L-16

Nqe lus piav qhia: A032Mo yog ib qho ultra-low carbon Cr19Ni13Mo3 stainless hlau electrode nrog titanium calcium txheej.Nws tuaj yeem siv rau AC thiab DC nrog cov txheej txheem ua haujlwm zoo.Kev tiv thaiv corrosion rau sulfuric acid, sulfurous acid thiab organic acid yog zoo dua li ntawm E316L.

Daim ntawv thov: Nws yog siv rau vuam tib yam ntawm stainless hlau cov ntaub ntawv xws li AISI317 thiab 317L steel, thiab kuj yog haum rau welding thiab surfacing corrosion-resistant khaubncaws sab nraud povtseg ntawm composite hlau thiab tshwj xeeb-zoo li tus hlau.

 

Tshuaj muaj pes tsawg leeg ntawm weld hlau (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤ 0.04

0.5 ~ 2.5 hli

≤0.90

18.0-21.0 Nws

12.0 ~ 14.0 Nws

3.0 ~ 4.0

≤ 0.75

≤ 0.030

≤ 0.040

 

Mechanical zog ntawm weld hlau:

Cov khoom kuaj

Tensile zog

Mpa

Elongation

%

lav

≥520

≥ 25

 

Pom zoo tam sim no:

Qws txoj kab uas hla

(mm)

2.0

2.5

3.2

4.0

5.0

Vuam tam sim no

(A)

25 ~ 50

50 ~ 80

80 ~ 110 ib

110 ~ 160 ib

160 ~ 220 ib

 

Daim ntawv ceeb toom:

1. Cov electrode yuav tsum tau ci rau 1 teev ntawm ib ncig ntawm 250 ℃ ua ntej vuam ua haujlwm;

2. Nws yog ib qho tseem ceeb los ntxuav cov xeb, roj nplai, dej, thiab impurities ntawm vuam qhov chaw ua ntej vuam.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, vuam rods, thiabvuam consumablesrau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.


  • Yav dhau los:
  • Tom ntej: