DIN 8555 (E6-UM-60) Hard Surfacing Vuam Qws, Hnav Resistant Vuam Electrode Arc Stick Electrode

Lus piav qhia luv luv:

DIN 8555 (E6-UM-60) yog ib qho yooj yim coated SMAW electrode rau tawv surfacing nrog zoo heev tiv thaiv compression stresses thiab cuam tshuam.


Product Detail

Khoom cim npe

Hardfacing Vuam Electrode

 

Txheem: DIN 8555 (E6-UM-60)

Hom No.: TY-C DUR 600

 

Specification & Daim Ntawv Thov:

· Basic coated SMAW electrode rau tawv nto.

· Zoo heev tiv thaiv compression kev nyuaj siab thiab cuam tshuam.

· Universally muaj feem xyuam rau cladding ntawm cov hlau, cam khwb cia hlau thiab siab Mn-steel, raug ib txhij rau abrasion, cuam tshuam thiab compression.Daim ntawv thov teb yog lub ntiaj teb txav thiab kho pob zeb kev lag luam, xws li cov hniav excavator, thoob riam, crusher puab tsaig thiab cones, zeb hammers thiab lwm yam.

 

Chemical muaj pes tsawg leeg ntawm deposited hlau (%):

 

C

Si

Mn

Cr

Mo

Nb

Ni

W

V

Fe

DIN

0.2

2.0

-

-

5.0

-

-

-

-

-

-

Bal.

EN

0.2

2.0

-

0.3

3.0

5.0

18.0 Nws

-

4.5

-

10

-

-

2.0

-

2.0

Bal.

Hom

0.50 ib

2.3

1.80 ib

9.0 ib

-

-

-

-

-

Bal.

 

 

Hardness ntawm deposited hlau:

Raws li Welded

(HRC)

Tom qab soft-annealing 780-820 ℃ / qhov cub

(HRC)

Tom qab hardening 1000-1050 ℃ / roj

(HRC)

1 txheej rau

siab Mn-steel

(HRC)

2 txheej on

siab Mn-steel

(HRC)

56–58 : kuv

25

60

22

40

 

Cov yam ntxwv dav dav:

· Microstructure Martensitic

· Machinability Zoo nrog tungsten carbides tipped cov cuab yeej

· Preheating Preheat qhov hnyav thiab siab dua-tensile steels rau 200-350 ℃

· Redrying Redry rau 2 h ntawm 300 ℃ ua ntej siv.