E410NiMo-15 vuam electrode

Kev Piav Qhia Luv:

E410NiMo-15 yog lub tshuab hluav taws xob martensitic stainless hlau vuam nrog cov hydrogen sodium tsawg-txheej 11.0-12.5% ​​Cr, 4.0-5.0 Ni, thiab 0.40-0.70% Mo.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Tus Qauv Sib Xws

GB/T 983-2012 E410NiMo-15

AWS A5.4M-2012 E410NiMo-15

Cov Khoom Siv Sib Npaug:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM, UNS S41500

Kev piav qhia

E410NiMo-15 yog ib lub hlau stainless hlau martensitic uas muaj cov txheej txheem sodium hydrogen tsawg, muaj 11.0-12.5% ​​Cr, 4.0-5.0% Ni, thiab 0.40-0.70% Mo. Nws tsim nyog rau txhua qhov chaw vuam hlau arc (SMAW) nrog arc ruaj khov, tsawg spatter, thiab zoo heev slag detachability. Cov hlau tso muaj lub zog siab, zoo corrosion tsis kam, thiab tawg tsis kam. Preheating yog pom zoo rau cov workpieces tuab, thiab post-weld cua sov kho (PWHT) ntawm 580 ~ 620 ℃ (1-2 teev, cua txias, AC) yog qhov yuav tsum tau ua.

Daim Ntawv Thov

Zoo tagnrho rau kev vuam ASTM CA6NM cam khwb cia hlau, 13% Cr-4% Ni series hlau (piv txwv li, Cr13Ni4Mo, Cr13Ni5Mo), thiab cov hlau tsis xeb martensitic zoo sib xws. Cov ntawv thov ib txwm muaj xws li kev kho vuam ntawm cov hydropower turbine runners, lub cev valve, cov kav dej siab, thiab kev ua kom cov khoom siv cavitation hnav. Kuj tseem siv rau kev kho cov khoom siv tawv tawv xws li cov crusher rolls thiab cov twj tso kua mis casings.

Cov Tshuaj Lom Zem ntawm Cov Hlau Weld (%)

Khoom C Mn Si P S Cr Ni Mo Cu
Qhov Yuav Tsum Tau Ua ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Cov txiaj ntsig ntawm kev xeem 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Cov Khoom Siv Kho Tshuab ntawm Cov Hlau Tso Tawm

Lub Npe Xeem Lub zog tensile (Mpa) Kev ntev% X-Ray Kev Ntsuas Qhov Cuam Tshuam, (+ 20 ℃) ​​J Qhov nyuaj HB Cov Hydrogen Uas Diffuse Tau (ml/100g)
Qhov Yuav Tsum Tau Ua ≥760 ≥15 Qib I – – ≤5
Cov txiaj ntsig ntawm kev xeem 845 19 Qib I 60-90 250-310 ≤5

Cov Kev Ntsuas Vuam Pom Zoo

Lub Hwj Chim Tau Los: DC Reserve (DC-)

Pom Zoo Tam Sim No

Qws Txoj Kab uas hla (hli) 3.2 4.0 5.0
Vuam Tam Sim No (A) 80-120 120-160 150-190

Daim Ntawv Ceeb Toom:

1. Ci lub electrode ntawm 300 ℃ rau ib teev ua ntej siv kom tshem tawm cov dej noo.
2. Ntxuav cov xeb, roj, thiab cov dej noo ntawm cov hlau puag; siv kev ua haujlwm luv luv rau cov hlaws weld nqaim.
3. PWHT yuav tsum tau ua tam sim ntawd tom qab vuam kom tsis txhob muaj embrittlement.

  • Yav dhau los: