E6013 (J421 / 422) cov hlau carbon electrode

Kev Piav Qhia Luv:

AWS A5.1 E6013(J421) yog ib hom electrode rutile.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Kev faib tawm:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Cov yam ntxwv:

AWS A5.1 E6013(J421) yog ib hom rutile electrode. Siv tau rau kev vuam ob qho tib si AC & DC fais fab thiab siv tau rau txhua qhov chaw. Nws muaj kev ua haujlwm vuam zoo heev xws li arc ruaj khov, me ntsis spatter, yooj yim tshem tawm slag thiab reignition-muaj peev xwm thiab lwm yam. Rutile-cellulosic electrode nrog lub peev xwm vuam zoo hauv txhua qhov chaw suav nrog ntsug nqes. Zoo heev gap-bridging thiab arc-striking muaj peev xwm. Rau tack vuam thiab load haum ups. Lub hom phiaj dav dav rau kev lag luam thiab kev lag luam, sib dhos thiab khw vuam.

Cov Tshuaj Lom Zem ntawm Txhua Cov Hlau Weld: (%)
Cov Tshuaj Lom Zem C Mn Si S P Ni Cr Mo V
Cov Kev Cai ≤0.10 0.32-0.55 ≤0.30 ≤0.030 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Cov Txiaj Ntsig Ib Txwm Muaj 0.08 0.37 0.18 0.020 0.025 0.030 0.035 0.005 0.004
Cov Khoom Siv Kho Tshuab ntawm Cov Hlau Tso Tawm
Khoom Siv Kuaj Rm (N/mm2) Rel (N/mm2) Ib (%) KV2 (J) 0 ℃
Cov Kev Cai 440-560 ≥355 ≥22 ≥47
Cov Txiaj Ntsig Ib Txwm Muaj 500 430 27 80
AWS A5.1 E6013 yog tsim rau kev vuam cov qauv ua los ntawm cov hlau tsis tshua muaj carbon, ua tau zoo heev hauv kev vuam cov hlau nyias thiab me me thiab kuj muaj kev ua tau zoo heev hauv qhov xwm txheej uas xav tau cov hlaws dai zoo nkauj thiab huv si.

Txoj Haujlwm Vuam:

PA, PB, PC, PD, PE, PF

Siv Tam Sim No (DC)
Txoj kab uas hla φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 80~ 130 150 ~ 210 180 ~ 240

Ceeb Toom:

Feem ntau, tsis txhob't yuav tsum rov ziab lub electrode ua ntej vuam. Thaum nws raug cuam tshuam los ntawm cov av noo, yuav tsum rov ziab nws ntawm 150℃-170℃rau 0.5-1 teev.


  • Yav dhau los:
  • Tom ntej no: