ENiCrFe-3 Electrodes rau Nickel

Kev Piav Qhia Luv:

Lub electrode tso 65Ni-20Cr-2Nb-1.5Mo weld hlau.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

EN ISO CODE: 14172:ENi6082

Lub electrode no muab 65Ni-20Cr-2Nb-1.5Mo vuam hlau tso rau hauv. Cov hlau vuam zoo li duab hluav taws xob uas muaj cov yam ntxwv zoo dua. Nws zoo tagnrho rau kev vuam cov hlau sib xyaw zoo sib xws, rau kev sib txuas cov hlau nrog Nickel-Chromium-Iron alloy thaum cov ntsiab lus Manganese siab tsis ua rau puas tsuaj, rau kev vuam sab ntawm Nickel Chromium-Iron clad steel thiab cov hlau sib xyaw ua ke. Haum rau kev sib tshooj ntawm cov phaj forge. Pom zoo tshwj xeeb rau kev vuam 9% Ni Steels rau kev pabcuam cryogenic. Kuj tseem siv rau kev vuam ntawm Nickel-Chromium alloys siv rau cov ntawv thov kub siab xws li cov khoom cua sov thiab cov raj reformer.

COV TSHUAJ YEEM SIB XYAW NTAWM TXHUA HLAU WELD

Khoom C Mn Si Cr Ni Fe Nb Cu Ti S P
Feem pua ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

COV CUAB YEEJ TXUJ CI IB TXWM NTAWM TXHUA HLAU WELD

UTS YS Kev ntev Lub zog cuam tshuam CVN (J) Kev nthuav dav sab nraud Lub zog nkag ntawm
(MPa) (MPa) (L = 5d)% ntawm qhov kub tsis tshaj 196°C ntawm -196°C (hli) 600 ° C rau 1000 teev.
620 500 30 75 0.85 160 MPa

COV NTAUB NTAWV TAM SIM NO THIAB COV NTAUB NTAWV UAS PACKING: DC (+)

Loj (hli)

Qhov ntev x qhov ntev

5 × 350

4 × 350

3.15 × 350

2.5 × 350

Qhov Ntau Tam Sim No (Amps)

150-180

120-150

80-110

60-70

Qhov hnyav/Thawv (kgs)

2.5

2.5

2.5

2.5

Kev ceev faj

1. Xyuas kom cov electrodes qhuav. Rov ziab cov electrodes ntawm 300-325°C rau ib teev.

2. Tswj kom muaj ib txoj kab luv luv, ib txoj hlua khi thiab txo qhov cua sov nkag.

3. Cia qhov vuam txias kom qis dua 50 C ua ntej tso nyiaj, txheej tom ntej.


  • Yav dhau los:
  • Tom ntej no: