ER70S2 yog hlau MIG & TiG zoo tshaj plaws rau kev vuam rau txhua qib ntawm cov hlau tsis hnyav thiab cov hlau carbon, tsim cov vuam zoo nrog qhov porosity tsawg kawg nkaus. Nws yog hlau triple deoxidized (Zirconium, Titanium, thiab Aluminium) ua rau nws yog qhov kev xaiv zoo heev rau kev vuam hla xeb thiab qhov ntsuas zeb. Tsis tas yuav muaj flux nrog cov khoom no.
COV NTAWV THOV IB TXWM:
cov kav dej thiab cov rigs drilling offshore, cov hlau ua haujlwm
| Txoj Haujlwm Vuam: F, V, OH, H | Tam sim no: DCEP |
| Lub zog tensile, kpsi: | 70 |
| Lub zog tawm los, kpsi: | 58 |
| Kev ntev hauv 2 "%: | 22 |
Ib txwm muaj Charpy V-Notch: 35 ft.-lb. Ntawm -20 deg F
Cov Khoom Siv Hluav Taws Xob Ib Txwm Muaj Raws Li AWS A5.18 (cov nqi ib qho yog qhov siab tshaj plaws)
| C | Mn | Si | P | S | Ni | Cr | Mo | V | Cu | Ti | Zr | Al | ||
| 0.07 | 0.90-1.40 | 0.40-0.70 | 0.025 | 0.035 | 0.15 | 0.15 | 0.15 | 0.03 | 0.50 | 0.05-0.15 | 0.02-0.12 | 0.05-0.15 | ||
| Cov Kev Ntsuas Vuam Ib Txwm Muaj | ||||||||||||||
| Txoj kab uas hla | Txheej Txheem | Volt | Cov Amps | Cov roj tiv thaiv | ||||||||||
| in | (hli) | |||||||||||||
| .035 | (0.9) | GMAW | 28-32 | 165-200 | Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2 | |||||||||
| .045 | (1.2) | GMAW | 30-34 | 180-220 | Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2 | |||||||||
| 1/16 | (1.6) | GMAW | 30-34 | 230-260 | Tshuaj tsuag hloov 98% Argon + 2% Oxygen lossis 75% Argon + 25% CO2 | |||||||||
| .035 | (0.9) | GMAW | 22-25 | 100-140 | Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO2 | |||||||||
| .045 | (1.14) | GMAW | 23-26 | 120-150 | Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO | |||||||||
| 1/16 | (1.6) | GMAW | 23-26 | 160-200 | Kev Hloov Pauv Luv Luv 100% CO2 lossis 75% Argon +25% CO | |||||||||
| .035 | (0.9) | GTAW | 13-16 | 60-100 | 100% Argon | |||||||||
| .045 | (1.14) | GTAW | 13-16 | 70-120 | 100% Argon | |||||||||
| 1/16 | (1.6) | GTAW | 12-15 | 100-125 | 100% Argon | |||||||||
| 3/32 | (2.4) | GTAW | 15-20 | 125-175 | 100% Argon | |||||||||
| 1/8 | (3.2) | GTAW | 15-20 | 175-250 | 100% Argon | |||||||||