Lus piav qhia luv luv:

ER-NiCrMo-4 yog siv rau kev vuam ntawm cov hlau uas muaj cov tshuaj zoo sib xws, qhov no suav nrog cov ntaub ntawv sib txawv ntawm cov nickel-base alloys, steels thiab stainless hlau.


Product Detail

Khoom cim npe

Nickel AlloyVuam HlauTig HlauERNiCrMo-4

 

Cov qauv
TS EN ISO 18274-Ni 6276-NiCr15Mo16Fe6W4
AWS A5.14 - ER NiCrMo-4

 

Nta thiab Daim Ntawv Thov

ER-NiCrMo-4 yog siv rau vuam ntawm cov hlau uas muaj cov tshuaj sib xws, qhov no suav nrog cov ntaub ntawv sib txawv ntawmnpib tsib xee-Base alloys, steels thiab stainless hlau.

Vim lub siab molybdenum cov ntsiab lus, cov alloy no muaj kev tiv thaiv zoo heev tiv thaiv kev ntxhov siab & corrosion cracking, pitting thiab crevice corrosion.

Feem ntau siv rau hauv cov kav dej, cov hlab ntsha siab, cov chaw ua tshuaj lom neeg, cov roj av sab nrauv, cov chaw siv roj, cov khoom siv hluav taws xob thiab cov chaw hauv dej hiav txwv thiab lwm yam.

Cov khoom siv hauv paus

N10276, W.Nr: 2.4819, NiMo16Cr15W, Alloy C4, Alloy C276*
* Cov lus piav qhia, tsis suav nrog cov npe

 

 

Tshuaj muaj pes tsawg leeg%
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 Nws 0.80 ib 0.70 ib 0.030 Nws 0.010 ib 0.75 ib  
             
Cu% Ni% Cov% Ti% Al%    
max 93.00 Nws max 2.00 Nws max    
0.20 ib min 1.00 Nws 3.50 Nws 1.00 Nws    

 

Mechanical Properties
Tensile zog ≥690 MPa  
Yield zog -  
Elongation -  
Kev cuam tshuam lub zog -  

Cov khoom siv tshuab yog kwv yees thiab yuav txawv raws li cov cua sov, tiv thaiv roj, vuam tsis thiab lwm yam.

 

Tiv thaiv Gases

TS EN ISO 14175 - TIG: I1 (Argon)

 

Vuam txoj hauj lwm

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Cov ntaub ntawv ntim
Txoj kab uas hla Ntev Qhov hnyav  
1.60 hli

2.40mm 3

3.20 mm

1000 hli

1000 hli

1000 hli

5 Kg

5 Kg

5 Kg

 