Nickel Alloy Vuam Hlau ERNiCrCoMo-1 Nickel Tig Hlau Filler Hlau

Lus piav qhia luv luv:

Alloy 617 (ERNiCrCoMo-1) yog cov hlau kub kub siv rau kev vuam nickel-chromium-cobalt-molybdenum alloys.


Product Detail

Khoom cim npe

Nickel AlloyVuam HlauTig HlauERNiCrCoMo-1

 

Cov qauv
TS EN ISO 18274-Ni 6617-NiCr22Co12Mo9
AWS A5.14 - ER NiCrCoMo-1

 

Nta thiab Daim Ntawv Thov

Alloy 617 yog cov hlau kub kub siv rau vuam ntawmnpib tsib xee-chromium-cobalt-molybdenum alloys.

Zoo tagnrho rau overlay cladding qhov uas zoo sib xws alloy yuav tsum tau, xws li roj turbines thiab ethylene khoom.

Haum rau kev koom nrog cov hlau tsis sib xws uas qhov kub siab zog thiab oxidation kuj yuav tsum tau txog li 1150 ° C.

Feem ntau siv rau hauv kev lag luam aerospace thiab lub zog tsim hluav taws xob, suav nrog cov nroj tsuag petrochemical rau kev siv xws li nitric acid catalyst daim phiaj thiab lwm yam.

Cov khoom siv hauv paus

Inconel alloys 600 thiab 601, Incoloy alloys 800 HT thiab 802 thiab cam khwb cia hlau xws li HK40, HP thiab HP45 Hloov kho.UNS Number N06617, 2.4663, 1.4952, 1.4958, 1.4959, NiCr21Co12Mo, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 NiCrAlTi 32 2081, Noy
* Cov lus piav qhia, tsis suav nrog cov npe

 

 

Tshuaj muaj pes tsawg leeg%

C%

Mn%

Fe%

P%

S%

Si%

Cu%

0.05 Nws

max

max

max

max

max

max

0.10

1.00 Nws

1.00 Nws

0.020 ib

0.015 ib

0.50 ib

0.50 ib

Ni%

Cov%

Al%

Ti%

Cr%

Mo%

44.00 Nws

10.00 Nws

0.80 ib

max

20.00 Nws

8.00 Nws

min

14.00 Nws

1.50 ib

0.60 ib

24.00 Nws

10.00 Nws

 

Mechanical Properties
Tensile zog ≥620 MPa
Yield zog -
Elongation -
Kev cuam tshuam lub zog -

Cov khoom siv tshuab yog kwv yees thiab yuav txawv raws li cov cua sov, tiv thaiv roj, vuam tsis thiab lwm yam.

 

Tiv thaiv Gases

TS EN ISO 14175 - TIG: I1 (Argon)

 

Vuam txoj hauj lwm

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Cov ntaub ntawv ntim

Txoj kab uas hla

Ntev

Qhov hnyav

1.60 hli

2.40mm 3

3.20 mm

1000 hli

1000 hli

1000 hli

5 Kg

5 Kg

5 Kg

 