ERCuSn-A (Phos Bronze A) Copper thiab Copper Alloy Bare Rods thiab Electrodes Tig thiab Mig Hlau

Lus piav qhia luv luv:

ERCuSn-A Phos Bronze A yog tooj liab-zinc bronze uas muaj kwv yees li 5% tin thiab mus txog 0.35% phosphorus ntxiv ua deoxidizer siv los vuam bronze thiab tooj dag.


Product Detail

Khoom cim npe

ERCuSn-A Phos Bronze A yog tooj liab-zinc bronze uas muaj kwv yees li 5% tin thiab mus txog 0.35% phosphorus ntxiv ua deoxidizer siv los vuam bronze thiab tooj dag.Nws kuj tseem siv tau los vuam tooj liab yog tias muaj cov tin nyob rau hauv cov hlau vuam tsis pom zoo.

Daim ntawv thov: overlaying steel;koom nrog 509-519 series tin-bronze puag hlau

AWS Class: ERCuSn-A Certification: AWS A5.7/A5.7M: 2007
Alloy: ERCuSn-A ASME SFA A5.7

 

Vuam txoj hauj lwm: Tam sim no:
AC-DCEP

 

Tensile zog, kpsi: 35
Brinell Hardness 70-85 : kuv

Hom Hlau Chemistry as per AWS A5.7 (tus nqi ib leeg yog siab tshaj)

Cu suav nrog Ag Al Pb P Sn Lwm yam
Tseem tshuav 0.01 ib 0.02 ib 0.10-0.35 dr hab 4.0-6.0 0.50 ib

 

Hom Vuam Parameters
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
1/16 (1.6) GTAW 70-120 : kuv 70-150 : kuv ACHF siv 100% Argon lossis Helium 2% Thoriated, Ceriated lossis Lanthanum Tungsten Electrode
3/32 (2.4) GTAW 120-160 : kuv 140-230 : kuv ACHF siv 100% Argon lossis Helium 2% Thoriated, Ceriated lossis Lanthanum Tungsten Electrode
1/8 (3.2) GTAW 170-230 : kuv 225-320 : kuv ACHF siv 100% Argon lossis Helium 2% Thoriated, Ceriated lossis Lanthanum Tungsten Electrode
Hom Vuam Parameters
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
0.035 ib (1.6) GMAW 20-26 100-200 100% Argon lossis 75% Argon, 25% Helium
0.045 ib (2.4) GMAW 22-28 100-250 100% Argon lossis 75% Argon, 25% Helium
1/16 (3.2) GMAW 29-32 : kuv 250-400 Nws 100% Argon lossis 75% argon, 25% Helium
3/32 (3.2) GMAW 32-34 : kuv 350-500 100% Argon lossis 75% Argon, 25% Helium

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 

 

 

 