D132 (B-83) Hardfacing Welding Electrode, Surfacing Vuam Qws, Arc Vuam Stick

Kev Piav Qhia Luv:

Cov electrode hydrogen qis rau kev tsim kho dua tshiab. Cov vuam tuaj yeem ua tshuab (tig, planed, milled, thiab lwm yam). Lub zog compressive siab. Zoo tiv taus kev puas tsuaj nruab nrab.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Hardfacing Vuam Stick ElectrodeRODO P

RODO PARA RECUBRIMIENTO PROTECTOR

Hom Naj Npawb:B – 83

Kev Tshuaj Xyuas Hlau Uas Tau Tso Tawm (Cov nqi ib txwm muaj)

C

0.1%

Mn

0.9%

Si

0.8%

Cr

3.2%

 

Cov yam ntxwv:

Cov electrode hydrogen qis rau kev tsim kho dua tshiab. Cov vuam tuaj yeem ua tshuab (tig, planed, milled, thiab lwm yam). Lub zog compressive siab. Zoo tiv taus kev puas tsuaj nruab nrab.

 

Cov Khoom Siv Kho Tshuab:Qhov nyuaj 27-31 HRc

 

Cov Haujlwm Vuam:Tiaj, Kab rov tav, Saum toj, Ntsug Saum.

 

Tam sim no thiab Polarity:

Rau kev hloov pauv lossis ncaj qha tam sim no

electrode rau tus ncej zoo

ø hli

ø nyob rau hauv

Amperage

3.20

1/8

110-130

4.00

5/32

140-180

5.00

2/16

190-240

 

Daim Ntawv Thov: Hauv cov menyuam pub, pulleys, khau nres.

• Txhawm rau sau cov sprockets ntawm cov tsheb laij teb

• Zoo heev ua lub hauv paus rau cov txheej tawv ntawm cov hlau carbon.

cov pa roj carbon

• Cov Trunnions, axles thiab caterpillars ntawm mechanical shovels.

• Cov thooj voos kheej kheej ntawm cov crusher

• Cov menyuam siv khoom

 

 

NTEV: 350 hli.

Qhov hnyav ib lub thawv: 20 kg/44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim muaj xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, cov pas nrig vuam, thiab cov khoom siv vuam rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb suav nrog cov hlau tsis xeb vuam electrodes, carbon hlau vuam electrodes, qis alloy vuam electrodes, surfacing vuam electrodes, nickel & cobalt alloy vuam electrodes, mild steel & low alloy vuam wires, stainless hlau vuam wires, gas-shielded flux cored wires, txhuas vuam wires, submerged arc vuam. wires, nickel & cobalt alloy vuam wires, tooj dag vuam wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, thiab lwm yam khoom siv vuam & khoom siv tau.

 

 

 

 


  • Yav dhau los:
  • Tom ntej no: