Hlau Vuam Hlau Nickel Alloy ENiFe-Cl Mig Vuam Hlau

Kev Piav Qhia Luv:

Ferro-nickel hlau khov kho siv rau kev vuam hlau cam khwb cia thiab hlau ductile.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Nickel AlloyHlau vuamENiFe-Cl

Cov Nta thiab Cov Ntawv Thov

Ferro-npib tsibhlau khov kho siv rau vuam hlau cam khwb cia thiab hlau ductile.

Haum rau cov pob qij sib txawv ntawm cov hlau cam khwb cia, hlau me me, hlau tsis tshua muaj alloy thiab hlau tsis xeb.

Pom zoo rau kev vuam cov castings uas muaj sulfur ntau, phosphorous lossis lubricant-contamination.

Kev txiav txheej txheem precision rau cov yam ntxwv pub hlau zoo dua.

Feem ntau siv rau ntau yam kev kho thiab kev tsim khoom, suav nrog kev tsim kho dua tshiab cov ncej, log, cov pob qij txha tseem ceeb ntawm cov hlau thiab cov hlau cam khwb cia thiab lwm yam

Cov Khoom Siv Hauv Paus Ib Txwm Muaj

Hlau grey cam khwb cia, malleable, nodular*
* Piav qhia xwb, tsis yog daim ntawv teev tag nrho

 

Cov Qauv
EN ISO 1071 – SC NiFe-1
AWS A5.15 – E NiFe-CI

 

Cov Tshuaj Muaj pes tsawg leeg%
C% Mn% Si% P% S%
siab tshaj plaws siab tshaj plaws siab tshaj plaws siab tshaj plaws siab tshaj plaws
2.00 0.80 0.20 0.03 0.03
Fe% Ni% Cu% Al%
rov qab. 54.00 siab tshaj plaws siab tshaj plaws
56.00 2.50 1.00

 

Cov Khoom Siv Kho Tshuab
Lub zog tensile 400 – 579 MPa
Lub Zog Tawm -
Kev ntev -
Lub zog cuam tshuam -

Cov khoom siv kho tshuab tsuas yog kwv yees xwb thiab tej zaum yuav txawv raws li qhov kub, roj tiv thaiv, cov txheej txheem vuam thiab lwm yam.

 

Cov Pa roj tiv thaiv

EN ISO 14175 - I1, Ar + 1-2% O2

 

Cov Haujlwm Vuam

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF

 

Cov Ntaub Ntawv Ntim Khoom
Txoj kab uas hla
Qhov hnyav Lub pob zeb PalletQhov ntau
1.20 hli 15 Kg BS300 72

Lub Luag Haujlwm:Txawm hais tias tau ua txhua yam kev siv zog los xyuas kom meej tias cov ntaub ntawv muaj nyob hauv, cov ntaub ntawv no yuav hloov pauv yam tsis tau ceeb toom thiab tsuas yog suav tias tsim nyog rau kev taw qhia dav dav xwb.

 