Hlau Nickel Alloy Vuam Hlau ERNiCu-7 Nickel Tig Hlau Filler Hlau

Kev Piav Qhia Luv:

ERNiCu-7 yog ib qho hlau nickel-tooj ​​liab uas tsim los rau kev vuam Monel.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Nickel AlloyHlau vuamTig HlauERNiCu-7

Cov Qauv
TS EN ISO 18274-Ni 4060 - NiCu30Mn3Ti
AWS A5.14 – ER NiCu-7

 

Cov Nta thiab Cov Ntawv Thov

Nickel-tooj ​​liab alloy tsim rau kev vuam Monel.

Zoo li cov hlaws dai zoo nkauj thiab zoo heev tiv taus corrosion hauv cov kua saline.

Cov hlau vuam muaj kev tiv taus zoo heev rau ntau yam corrosive media.

Cov hlau no kuj tseem siv rau kev vuam overlay.

Feem ntau siv rau hauv kev tsim kho hauv hiav txwv, tshwj xeeb tshaj yog nyob rau ntawm ntug dej hiav txwv, cov khoom sib pauv cua sov, cov kav dej, cov chaw ua dej ntsev, cov tshuaj lom neeg, petrochemical thiab kev lag luam hluav taws xob thiab lwm yam.

Cov Khoom Siv Hauv Paus Ib Txwm Muaj

Monel alloys 400 thiab 404 *
* Piav qhia xwb, tsis yog daim ntawv teev tag nrho

 

 

Cov Tshuaj Muaj pes tsawg leeg%

C%

Mn%

Fe%

P%

S%

Si%

siab tshaj plaws

3.00

0.50

siab tshaj plaws

siab tshaj plaws

siab tshaj plaws

0.15

4.00

2.50

0.020

0.015

1.00

Cu%

Ni%

Co%

Ti%

Al%

Nb+Ta%

28.00

62.00

siab tshaj plaws

1.50

siab tshaj plaws

siab tshaj plaws

32.00

69.00

1.00

3.00

1.00

0.50

 

Cov Khoom Siv Kho Tshuab
Lub zog tensile ≥450 MPa
Lub Zog Tawm ≥180 MPa
Kev ntev ≥30%
Lub zog cuam tshuam ≥80 J

Cov khoom siv kho tshuab tsuas yog kwv yees xwb thiab tej zaum yuav txawv raws li qhov kub, roj tiv thaiv, cov txheej txheem vuam thiab lwm yam.

 

Cov Pa roj tiv thaiv

TS EN ISO 14175 - TIG: I1 (Argon)

 

Cov Haujlwm Vuam

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Cov Ntaub Ntawv Ntim Khoom

Txoj kab uas hla

Ntev

Qhov hnyav

1.60 hli

2.40 hli

3.20 hli

1000 hli

1000 hli

1000 hli

5 Kg

5 Kg

5 Kg

 

Lub Luag Haujlwm: Txawm hais tias tau ua txhua yam kev rau siab kom ntseeg tau tias cov ntaub ntawv muaj tseeb, cov ntaub ntawv no yuav hloov pauv yam tsis tau ceeb toom thiab tsuas yog suav tias yog qhov tsim nyog rau kev taw qhia dav dav.


  • Yav dhau los:
  • Tom ntej no: