AWS E8010-G Low Alloy Steel Welding Electrode, Best Welding Materials Supplier

Lus piav qhia luv luv:

J555G (AWS E8010-G) is a high cellulose sodium-coated vertical down electrode.


Product Detail

Khoom cim npe

Tsawg Alloy Steel Vuam Electrode

j555g ua                                               

GB/T E5510-G

AWS A5.5 E8010-G

Nqe lus piav qhia: J555G yog lub siab cellulose sodium-coated ntsug down electrode.Siv DCEP (direct tam sim no electrode zoo).Nws yog haum rau tag nrho txoj hauj lwm ntsug downward welding ntawm ncig seam ntawm lub raj xa dej.Nws tuaj yeem welded ntawm ib sab thiab tsim ntawm ob sab, thiab vuam ceev yog ceev.

Daim ntawv thov: Siv rau girth welding ntawm ntau yam tsawg alloy steel kav.

 

Tshuaj muaj pes tsawg leeg ntawm weld hlau (%):

C

Mn

Si

S

P

≤ 0.20

≥1.00 Nws

≤0.50

≤ 0.035

≤ 0.035

 

Mechanical zog ntawm weld hlau:

Cov khoom kuaj

Tensile zog

Mpa

Yield zog

Mpa

Elongation

%

Tus nqi cuam tshuam (J)

-30 ℃

lav

≥540

≥440

≥17

≥ 27

X-ray kuaj: qib II

 

Pom zoo tam sim no:

(mm)

Qws txoj kab uas hla

2.5

3.2

4.0

5.0

(A)

Vuam tam sim no

40 ~ 70

70 ~ 110 ib

110 ~ 160 ib

160-190 ib

 

Daim ntawv ceeb toom:

1. Unpack lub vuam pas nrig ua ntej siv, thiab siv nws kom ntau li ntau tau tom qab unpacking;

2. Feem ntau, tsis tas yuav ziab nws dua ua ntej vuam, thiab nws tuaj yeem qhuav ntawm 70 ~ 90 ° C rau 1 teev thaum nws ntub.

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim khoom ntawmvuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon hlau vuam electrodes,low alloy vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, txhuas vuam hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 