Low Alloy Steel Welding Electrode J506NiMA, J507NiMA GB/T E5016-G E5015-G AWS E7018-G E7015-G

Lus piav qhia luv luv:

J506NiMA (AWS E7018-G) and J507NiMA (AWS E7015-G) is a moisture-absorbing ultra-low hydrogen-coated low-alloy steel electrodes.


Product Detail

Khoom cim npe

Tsawg Alloy Steel Vuam Electrode

J506NiMA, J507NiMA                                                     

GB/T E5016-G E5015-G

AWS E7018-G E7015-G

Nqe lus piav qhia: J506NiMA thiab J507NiMA yog cov dej noo-absorbing ultra-low hydrogen-coated low-alloy steel electrodes.Cov hlau deposited muaj zoo heev plasticity, tsawg-kub toughness thiab tawg tsis kam, thiab yuav welded nyob rau hauv txhua txoj hauj lwm.Cov txheej yog resistant rau noo noo nqus.Tom qab cov electrode tau ci ntawm 400 ° C x 1h thiab nres hauv ib puag ncig nrog cov av noo txheeb ze ≥ 80% rau 4 teev, cov dej noo ntawm cov txheej tseem ua tau raws li qhov yuav tsum tau siv.

Daim ntawv thov: Nws yog siv rau kev vuam ntawm cov roj platforms, nkoj, cov hlab ntsha siab, thiab lwm yam qauv ua los ntawmcarbon steel thiab low alloy steel.

 

Tshuaj muaj pes tsawg leeg ntawm weld hlau (%):

C

Mn

Si

Ni

S

P

lav

≤0.12

≥1.00 Nws

≤0.50

≤ 0.60

≤ 0.035

≤ 0.040

 

Mechanical zog ntawm weld hlau:

Cov khoom kuaj

Tensile zog

Mpa

Yield zog

Mpa

Elongation

%

Tus nqi cuam tshuam (J)

-46 ℃

lav

≥490

≥390

≥ 22

≥ 27

 

Diffusion hydrogen ntsiab lus ntawm deposited hlau: ≤5.0mL / 100g (gas chromatography los yog mercury method)

Cov dej noo ntawm electrode txheej: ≤0.30%

X-ray kuaj: qib kuv

 

Pom zoo tam sim no:

Qws txoj kab uas hla

2.5

3.2

4.0

5.0

Vuam tam sim no

60 ~ 90

90 ~ 120 hli

140 ~ 180 ib

170-210 ib

 

Daim ntawv ceeb toom:

1. Cov electrode yuav tsum tau ci rau 1 teev ntawm 350 ~ 400 ℃ ua ntej vuam ua haujlwm;

2. Nws yog ib qho tseem ceeb los ntxuav cov xeb, roj nplai, dej, thiab impurities ntawm vuam qhov chaw ua ntej vuam;

3. Siv luv arc ua haujlwm thaum vuam.Txoj kev nqaim welding yog tsim nyog.

 