AWS E7015 Welding Rods

Lus piav qhia luv luv:

AWS A5.1 E7015 is low-hydrogen sodium coated carbon steel electrode.


Product Detail

Khoom cim npe

AWS A5.1 E7015 is low-hydrogen sodium coated carbon steel electrode.

E7015 vuam electrode yuav tsum tau ua ntawm DCEP.Nws muaj cov vuam siv tau zoo heev uas ua rau nws ua tau txhua txoj haujlwm vuam, muaj qhov ruaj khov arc, tshem tawm ntawm slag yog ib qho yooj yim thiab tsis muaj spatter.Cov hlau deposited muaj zoo mechanical kev ua tau zoo thiab tawg-ua hauj, uas muaj zoo kub tsis tshua muaj toughness.

Daim ntawv thov

AWS A5.1 E7015 yog siv nyob rau hauv vuam nruab nrab-carbon steel thiab low-alloy lug xws li 16Mn, 09Mn2Si, 09Mn2V thiab cov hlau siv nyob rau hauv shipbuilding xws li A, B, D, E. Nws kuj yog siv nyob rau hauv tuab steel daim hlau thiab cov carbon steel qauv uas nyuaj rau weld.

Raws li Standard

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A

Lub hom phiaj: AWS A5.1 E7015 yog siv rau hauv vuam nruab nrab-carbon steel thiab qis-alloy qauv xws li 16Mn, 09Mn2Si, 09Mn2V thiab cov hlau siv hauv nkoj tsim xws li A, B, D, E. Nws kuj tseem siv rau cov hlau tuab. daim hlau thiab cov qauv carbon steel uas nyuaj rau vuam.

Chemical Composition (%)

Tshuaj muaj pes tsawg leeg

C

Mn

Si

S

P

Ni

Cr

Mo

V

Guarantee Tus nqi

≤

0.15

≤

1.60 ib

≤

0.90 ib

≤ 0.035

≤ 0.035

≤

0.30 Nws

≤

0.20 ib

≤

0.30 Nws

≤

0.08 ib

General Result

0.082 ib

1.10

0.58 ib

0.012 ib

0.021 ib

0.011 ib

0.028 ib

0.007 ib

0.016 ib

Mechanical Properties of Deposited Hlau (Shielding Gas: CO2)

Cov khoom kuaj

Rm (MPa)

ReL (MPa)

A(%)

KV2 (J)

-20 ℃ -30 ℃

Guarantee Tus nqi

≥490

≥400

≥ 20

≥47

≥ 27

General Result

550

450

32

150

142

X-Ray Radio-graphic Test Requirements: Qib I

Kev siv tam sim no (DC +)

Txoj kab uas hla (mm)

Φ2.5

Φ3.2

Φ4.0 ua

Φ5.0 ua

Amperage (A)

60 ~ 100

80-140 Nws

110-210 : kuv

160-230 Nws

Nco tseg:

1. Cov electrode yuav tsum tau preheated ntawm qhov kub ntawm 350 ° C rau 1 teev.Preheat tus pas nrig thaum twg nws siv.

2. Cov impurities xws li xeb, roj stains thiab ya raws yuav tsum tau muab tshem tawm ntawm cov khoom ua haujlwm.

3. luv arc yuav tsum tau ua vuam.Txoj kev nqaim weld yog nyiam.