AWS E9016-D1 Qis Alloy Steel Vuam Electrode J606 Vuam Rods GB/T E6016-D1

Kev Piav Qhia Luv:

J606 (AWS E9016-D1) yog cov hlau electrode uas muaj zog tsawg thiab muaj cov txheej potassium hydrogen tsawg. Nws siv tau rau kev vuam txhua qhov chaw nrog AC thiab DC. Kev ruaj khov ntawm AC vuam tsis zoo li DC vuam.


Cov Lus Qhia Txog Khoom

Cov Cim Npe Khoom

Cov Hlau Sib Txuas Qis

J606                                       

GB/T E6016-D1

AWS E9016-D1

Kev piav qhia: J606 yog cov hlau electrode uas muaj zog tsawg nrog cov txheej txheem potassium hydrogen tsawg. Nws tuaj yeem siv rau kev vuam txhua qhov chaw nrog AC thiab DC. Kev ruaj khov ntawm AC vuam tsis zoo li DC vuam.

Daim Ntawv Thov: Siv rau kev vuam cov hlau carbon nruab nrab thiab cov hlau tsis tshua muaj zog uas muaj zog sib xws, xws li Q420, thiab lwm yam.

 

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm cov hlau vuam (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Cov khoom siv kho tshuab ntawm cov hlau vuam:

Khoom sim

Lub zog tensile

Mpa

Lub zog tawm los

Mpa

Kev ntev

%

Tus nqi cuam tshuam (J)

-30 ℃

Tau lees paub

≥590

≥490

≥15

≥27

Tau kuaj xyuas

620 ~ 680

≥500

20 ~ 28

≥27

 

Cov ntsiab lus hydrogen diffusion ntawm cov hlau tso: ≤4.0mL / 100g (txuj ci glycerin)

Kev tshuaj xyuas X-ray: Kuv qib

 

Pom zoo tam sim no:

(hli)

Txoj kab uas hla ntawm tus pas nrig

2.0

2.5

3.2

4.0

5.0

5.8

(Ib)

Vuam Tam Sim No

40 ~ 70

70 ~ 90

90 ~ 120

140 ~ 180

180 ~ 220

210 ~ 260

 

 

Daim Ntawv Ceeb Toom:

1. Lub electrode yuav tsum tau ci rau 1 teev ntawm 350 ℃ ua ntej vuam ua haujlwm;

2. Nws yog ib qho tseem ceeb uas yuav tsum tau ntxuav cov xeb, roj nplai, dej, thiab cov khoom tsis huv ntawm cov khoom vuam ua ntej vuam;

3. Siv lub voj voog luv luv thaum vuam. Txoj kev vuam nqaim yog qhov tsim nyog;

4. Thaum qhov chaw vuam tuab, nws yuav tsum tau preheated rau saum 150 ° C thiab txias maj mam tom qab vuam.

 