Nickel AlloyHlau vuamTig HlauERNiCrMo-3
Cov Nta thiab Cov Ntawv Thov
Siabnpib tsibhlau alloy tsim rau kev vuam thiab claddingnpib tsib-raws li cov hlau sib xyaw xws li 625 lossis cov khoom zoo sib xws.
Kos duab khov kho hauv txoj kev tshwj xeeb heev kom tau txais cov vuam huv dua thiab zoo dua nrog cov kab sib txuas ci ntsa iab thiab ductility zoo heev.
Cov hlau vuam muaj cov khoom siv kho tshuab zoo heev ntawm qhov kub siab thiab qis.
Zoo tiv taus kev pitting thiab kev ntxhov siab corrosion.
Qhov kub ua haujlwm pom zoo yog txij li cryogenic mus txog 540 ° C.
Feem ntau siv rau hauv kev lag luam tshuaj lom neeg, kev tsim kho dej hiav txwv, cov khoom siv nuclear reactor, aerospace thiab hauv cov khoom siv tswj kev ua qias tuaj thiab lwm yam.
Cov Khoom Siv Hauv Paus Ib Txwm Muaj
Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926*
* Piav qhia xwb, tsis yog daim ntawv teev tag nrho
| Cov Qauv |
| TS EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb |
| AWS A5.14 – ER NiCrMo-3 |
| Cov Tshuaj Muaj pes tsawg leeg% | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | Cu% |
| siab tshaj plaws | siab tshaj plaws | siab tshaj plaws | siab tshaj plaws | siab tshaj plaws | siab tshaj plaws | siab tshaj plaws |
| 0.10 | 0.50 | 0.50 | 0.015 | 0.015 | 0.50 | 0.50 |
|
|
|
|
|
|
|
|
| Ni% | Co% | Al% | Ti% | Cr% | Nb+Ta% | Mo% |
| 60.00 | siab tshaj plaws | siab tshaj plaws | siab tshaj plaws | 20.00 | 3.15 | 8.00 |
| feeb | 1.0 | 0.40 | 0.40 | 23.00 | 4.15 | 10.00 |
| Cov Khoom Siv Kho Tshuab | ||
| Lub zog tensile | ≥760 MPa | |
| Lub Zog Tawm | ≥415 MPa | |
| Kev ntev | ≥35% | |
| Lub zog cuam tshuam | ≥100 J | |
Cov khoom siv kho tshuab tsuas yog kwv yees xwb thiab tej zaum yuav txawv raws li qhov kub, roj tiv thaiv, cov txheej txheem vuam thiab lwm yam.
Cov Pa roj tiv thaiv
TS EN ISO 14175 - TIG: I1 (Argon)
Cov Haujlwm Vuam
TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG
| Cov Ntaub Ntawv Ntim Khoom | |||
| Txoj kab uas hla | Ntev | Qhov hnyav | |
| 1.60 hli 2.40 hli 3.20 hli | 1000 hli 1000 hli 1000 hli | 5 Kg 5 Kg 5 Kg | |
Lub Luag Haujlwm: Txawm hais tias tau ua txhua yam kev rau siab kom ntseeg tau tias cov ntaub ntawv muaj tseeb, cov ntaub ntawv no yuav hloov pauv yam tsis tau ceeb toom thiab tsuas yog suav tias yog qhov tsim nyog rau kev taw qhia dav dav.