W707Ni Tsis tshua muaj kub Steel Vuam Electrode Tsawg-Hydrogen Stick Vuam Lwm tus neeg

Lus piav qhia luv luv:

W707Ni yog cov hlau tsis tshua muaj hluav taws xob uas muaj Ni hauv cov txheej txheem hydrogen sodium tsawg.


Product Detail

Khoom cim npe

Tsawg kub hlauVuamHluav taws xob

wb 707ni                                                     

GB/T E5515-C1

Nqe lus piav qhia: W707Ni yog cov hlau tsis tshua muaj hluav taws xob uas muaj Ni hauv cov txheej txheem hydrogen sodium tsawg.Siv DCEP (cov khoom siv hluav taws xob ncaj qha tam sim no) thiab tuaj yeem txuas rau txhua txoj haujlwm.Cov hlau tso tawm tseem muaj qhov cuam tshuam zoo ntawm -70 ° C.

Daim ntawv thov: Siv rau vuam tsis tshua muaj hlau xws li 2.5Ni.

 

Tshuaj muaj pes tsawg leeg ntawm weld hlau (%):

C

Mn

Si

Ni

S

P

≤ 0.12

≤1.25

≤ 0.60

2.00-2.75 Nws

≤ 0.020

≤ 0.025

 

Mechanical zog ntawm weld hlau:

Cov khoom kuaj

Tensile zog

Mpa

Yield zog

Mpa

Elongation

%

Tus nqi cuam tshuam (J)

-70 ℃

lav

≥540

≥440

≥17

≥ 27

 

Diffusion hydrogen ntsiab lus ntawm deposited hlau: ≤6.0mL / 100g (glycerin method) los yog ≤10mL / 100g (mercury los yog gas chromatography method)

X-ray kuaj: qib kuv

 

Pom zoo tam sim no:

(mm)

Qws txoj kab uas hla

2.0

2.5

3.2

4.0

5.0

(A)

Vuam tam sim no

40 ~ 70

60 ~ 90

90 ~ 120 hli

140 ~ 180 ib

170-210 ib

 Daim ntawv ceeb toom:

  1. Cov electrode yuav tsum tau ci rau 1 teev ntawm 350 ℃ ua ntej vuam ua haujlwm;
  2. Nws yog ib qho tseem ceeb los ntxuav cov xeb, roj nplai, dej, thiab impurities ntawm vuam qhov ua ntej vuam;
  3. Sim siv cov kab me me zog thaum vuam, ntau txheej thiab ntau dhau vuam.

 