ER1100 A5.10 Txhuas Kab tshoob Hlau Mig Rods thiab Electrodes

Lus piav qhia luv luv:

ER1100 tiv taus tshuaj lom neeg thiab huab cua.Nws yog ib tug kuj mos alloy uas yog heev formable thiab yog siv feem ntau nyob rau hauv nyias gauge thiab ntawv ci khoom.


Product Detail

Khoom cim npe

ER1100 A5.10, ALUMINIUM THIAB ALUMINIUM ALLOY Electrodes thiab Rods

ER1100 tiv taus tshuaj lom neeg thiab huab cua.Nws yog ib tug kuj mos alloy uas yog heev formable thiab yog siv feem ntau nyob rau hauv nyias gauge thiab ntawv ci khoom.Nws muaj cov yam ntxwv zoo wetting thiab nws kuj yog siv los ua ib qho khoom siv rau vuam lub hom phiaj.Cov yam ntxwv zoo ntawm cov hlau yog qhov ci tiav tau los ntawm anodizing.

Daim ntawv thov: tshav kub exchanger;khoom siv tuav zaub mov;rivets;khi hlau;metalizing

AWS: ER1100 Certification: AWS A5.10/A5.10M:1999
Hlau alloy: ER1100 AWS/ASME SFA A5.10

 

Vuam txoj hauj lwm:
F, V, OH, H
Tam sim no:
DCEP-GMAW
AC-GTAW

 

Yam khoom (raws li welded)

conductivity: 59% IACS (-12)
Tensile zog, kpsi: 13
Xim: Grey
Melting Point 1215 ⁰ F Solidification 1090 ⁰ F Qhov ntom 0.098 lbs/cu Ib.

Hom Hlau Chemistry as per AWS A5.10 (tus nqi ib leeg yog siab tshaj)

Si + Fe Cu Mn Zn Lwm yam Al  
0.95 ib 0.05-0.20 Nws 0.05 Nws 0.10 0.15 99,0 nqi  
Hom Vuam Parameters
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
.030 ib (.8) GMAW 15-24 60-175 : kuv Argon (hli)
.035 ib (.9) GMAW 15-27 70-185 : kuv Argon (hli)
3/64" (1.2) GMAW 20-29 125-260 : kuv Argon (hli)
1/16" (1.6) GMAW 24-30 : kuv 170-300 Nws Argon (hli)
3/32 " (2.4) GMAW 26-31 : kuv 275-400 Nws Argon (hli)
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
1/16" (1.6) GTAW 15 60-80 Argon (hli)
3/32 " (2.4) GTAW 15 125-160 : kuv Argon (hli)
1/8 " (3.2) GTAW 15 190-220 : kuv Argon (hli)
5/32" (4.0) GTAW 15 200-300 Argon (hli)
3/16" (4.8) GTAW 15-20 330-380 : kuv Argon (hli)

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 

 


  • Yav dhau los:
  • Tom ntej: