ER4043 Aluminium thiab Aluminium Alloy Vuam Hlau Tig thiab Mig Vuam Hlau

Lus piav qhia luv luv:

ER4043 yog lub hom phiaj dav dav ntawm txhuas vuam hlau.Nws yog ib qho ntawm cov qub thiab feem ntau siv vuam thiab brazing alloys.


Product Detail

Khoom cim npe

ER4043 yog lub hom phiaj dav dav ntawm txhuas vuam hlau.Nws yog ib qho ntawm cov qub thiab feem ntau siv vuam thiab brazing alloys.Qhov no aluminium alloy muaj cov khoom siv silicon, uas ua rau muaj kev txhim kho fluidity (wetting action) ntawm lub pas dej ua ke thiab tseem ua rau lub vuam tsis tshua muaj kev sib tsoo.Nws ci weld tiav ua rau nws yog ib qho kev xaiv nrov ntawm welders.ER4043 tuaj yeem siv los txuas ntau qib ntawm txhuas.

Daim ntawv thov: vuam muab tub lim;tshuaj tsuag thiab nplaim metalizing hlau

AWS: ER4043 Certification: AWS A5.10/A5.10M:1999
Hlau alloy: ER4043 AWS/ASME SFA A5.10

 

Vuam txoj hauj lwm:
F, V, OH, H
Tam sim no:
DCEP-GMAW
AC-GTAW

 

Yam khoom (raws li welded)

conductivity: 42% IACS (-12)
Tensile zog, kpsi: 29
Xim: Grey
Melting Point 1170 ⁰ F Solidification 1065 F Qhov ntom 0.097 lbs/cu In.

Hom Hlau Chemistry as per AWS A5.10 (tus nqi ib leeg yog siab tshaj)

Si Fe Cu Mn Mg Zn Ti Lwm yam Al
4.5-6.0 Nws 0.8 ua 0.30 Nws 0.05 Nws 0.05 Nws 0.10 0.20 ib 0.15 Tseem tshuav
Hom Vuam Parameters
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
.030 ib (.8) GMAW 15-24 60-175 : kuv Argon (hli)
.035 ib (.9) GMAW 15-27 70-185 : kuv Argon (hli)
3/64" (1.2) GMAW 20-29 125-260 : kuv Argon (hli)
1/16" (1.6) GMAW 24-30 : kuv 170-300 Nws Argon (hli)
3/32 " (2.4) GMAW 26-31 : kuv 275-400 Nws Argon (hli)
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
1/16" (1.6) GTAW 15 60-80 Argon (hli)
3/32 " (2.4) GTAW 15 125-160 : kuv Argon (hli)
1/8 " (3.2) GTAW 15 190-220 : kuv Argon (hli)
5/32" (4.0) GTAW 15 200-300 Argon (hli)
3/16" (4.8) GTAW 15-20 330-380 : kuv Argon (hli)

 

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 

 