Lus piav qhia luv luv:

ER5356 yog lub hom phiaj dav dav ntawm aluminium alloy uas feem ntau xaiv rau nws lub zog siab shear.


Product Detail

Khoom cim npe

ER5356 yog lub hom phiaj dav dav ntawm aluminium alloy uas feem ntau xaiv rau nws lub zog siab shear.Tsis tas li ntawd, nws kuj muaj kev tiv thaiv corrosion zoo heev thaum raug dej ntsev.ER5356 yuav tsum tau txiav txim siab rau vuam 5000 series aluminium puag hlau.

Daim ntawv thov: vuam muab tub lim

AWS: ER5356 Certification: AWS A5.10/A5.10M:1999
Hlau alloy: ER5356 AWS/ASME SFA A5.10
Vuam txoj hauj lwm:
F, V, OH, H
Tam sim no:
DCEP-GMAW
AC-GTAW
Yam khoom (raws li welded)
conductivity: 29% IACS (-0) / 27% IACS (-H18)
Tensile zog, kpsi: 38
Xim: Dawb
Melting Point 1175 ⁰ F Solidification 1060 F Qhov ntom 0.096 lbs/cu In.
Hom Hlau Chemistry as per AWS A5.10 (tus nqi ib leeg yog siab tshaj)
Si Fe Cu Mn Mg Cr Zn Ti Lwm yam AL
0.25 0.40 Nws 0.10 0.50-1.0 Nws 4.7-5.5 0.05-0.20 Nws 0.25 0.05-0.20 Nws 0.15 Tseem tshuav
Hom Vuam Parameters
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
.030 ib (.8) GMAW 15-24 60-175 : kuv Argon (hli)
.035 ib (.9) GMAW 15-27 70-185 : kuv Argon (hli)
3/64" (1.2) GMAW 20-29 125-260 : kuv Argon (hli)
1/16" (1.6) GMAW 24-30 : kuv 170-300 Nws Argon (hli)
3/32 " (2.4) GMAW 26-31 : kuv 275-400 Nws Argon (hli)
Txoj kab uas hla Txheej txheem Volt Amps GAS
in (mm)
1/16" (1.6) GTAW 15 60-80 Argon (hli)
3/32 " (2.4) GTAW 15 125-160 : kuv Argon (hli)
1/8 " (3.2) GTAW 15 190-220 : kuv Argon (hli)
5/32" (4.0) GTAW 15 200-300 Argon (hli)
3/16" (4.8) GTAW 15-20 330-380 : kuv Argon (hli)

Wenzhou Tianyu Electronic Co., Ltd. tau tsim nyob rau xyoo 2000. Peb tau koom nrog kev tsim cov vuam electrodes, vuam rods, thiab vuam consumables rau ntau tshaj 20 xyoo.

Peb cov khoom tseem ceeb muaj xws li stainless hlau vuam electrodes, carbon steel vuam electrodes, tsis tshua muaj hlau vuam electrodes, surfacing vuam electrodes, npib tsib xee & cobalt alloy vuam electrodes, me steel & tsawg alloy vuam hlau, stainless hlau vuam hlau, roj-shielded flux cored nyob ntawm tej, aluminium welding hlau, submerged arc vuam.Cov xov hlau, npib tsib xee & cobalt alloy vuam hlau, tooj dag vuam hlau, TIG & MIG vuam hlau, tungsten electrodes, carbon gouging electrodes, thiab lwm yam vuam accessories & consumables.

 

 